Patents
US 7,695,703 B2#18800842 Most CitedActiveUnited States (USPTO)Utility

High temperature catalyst and process for selective catalytic reduction of NOx in exhaust gases of fossil fuel combustion

6Forward Citations (#18800842 Global)
0.4/yrCitation Velocity (#21306418 Global)
1.27Citation PageRank (#29657324 Global)
14Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A process for producing a stable high-temperature catalyst for reduction of nitrogen oxides in combustion exhaust gases at operating temperatures from 300° C. to over 700° C. without the need for exhaust dilution. A zeolite material is steam-treated at a temperature and duration sufficient to partially de-aluminize the zeolite to approximately a steady state, but not sufficient to fully collapse its chemical structure. Iron is added to the zeolite material. The zeolite material is calcined at a temperature, humidity, and duration sufficient to stabilize the zeolite material. Examples and specifications for ranges, order, and durations of steaming, calcining, and other steps are provided.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 6.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process of selective catalytic reduction of NOx in a combustion exhaust stream comprising: preparing a catalyst by the steps of a) steam treating a zeolite material at about 500° C.-600° C. for about 5-15 hours; b) adding iron to the zeolite material at a loading between 0.01% and 10% iron; and c) calcining the zeolite material at about 750° C.-900° C. for about 1-5 hours; wherein the order of steps a) and b) may vary, followed by step c); mixing 60-82 ppm of ammonia into a combustion exhaust stream at over 500° C.; contacting the combustion exhaust stream at 500° C.-650° C. with the catalys

  2. Claim 2Independent Claim

    A process for preparing a catalyst for reduction of NOx in combustion exhaust, comprising: a) steam treating a zeolite material at about 500° C.-60

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • Chi-Cheng Liu, Hsisheng Teng; "Cu/MCM-41 for selective catalytic NO reduction with NH3-comparison of different Cu-loading methods"; Applied Catalysis B: Environmental 58; Jan. 4, 2005; pp. 69-77; Elsevier B.V.
  • Gerard Delahay, Stephane Kieger, Nathalie Tanchoux, Philippe Trens, Bernard Coq; "Kinetics of the selective catalytic reduction of NO by NH3 on a Cu-faujasite catalyst"; Applied Catalysts B: Enviromental 52; Jun. 2, 2004; pp. 251-257; Elsevier B.V.
  • Gongshin Qi, Ralph T. Yang; "Ultra-active Fe/ZSM-5 catalyst for selective catalytic reduction of nitric oxide with ammonia" ; Applied Catalysis B: Environmental 60; Mar. 16, 2005; pp. 13-22; Elsevier B.V.
  • Kevin J. Rogers; "SCR Inlet Maldistributions-Their Effects & Strategies for Their Control"; Proceedings of the 2002 Conference on Selective Catalytic Reduction and Selective Non-Catalytic Reduction for NOx Control; Presented in the US; May 15-16, 2002; Published by the National Energy Technology Lab
  • R.Q. Long and R.T. Yang; "Selective Catalytic Reduction of NO with Ammonia over Fe3+-Exchanged Mordenite (Fe-MOR): Catalytic Performance, Characterization, and Mechanistic Study"; Journal of Catalysis 207; 2002; pp. 274-285; Elsevier Science, USA.