Patents
US 7,687,799 B2#21749293 Most CitedActiveUnited States (USPTO)Utility

Methods of forming buffer layer architecture on silicon and structures formed thereby

5Forward Citations (#21749293 Global)
0.3/yrCitation Velocity (#25262892 Global)
1.33Citation PageRank (#27540060 Global)
2Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Methods and associated structures of forming a microelectronic device are described. Those methods may include forming a GaSb nucleation layer on a substrate, forming a Ga(Al)AsSb buffer layer on the GaSb nucleation layer, forming an In 0.52 Al 0.48 As bottom barrier layer on the Ga(Al)AsSb buffer layer, and forming a graded In x Al 1-x As layer on the In 0.52 Al 0.48 As bottom barrier layer thus enabling the fabrication of low defect, device grade InGaAs based quantum well structures.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 5.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method comprising: forming a GaSb nucleation layer on a substrate; forming a Ga(Al)AsSb buffer layer on the GaSb nucleation layer; forming an In 0.52 Al 0.48 As bottom barrier layer on the Ga(Al)AsSb buffer layer; and forming a graded In x Al 1-x As layer on the In 0.52 Al 0.48 As bottom barrier layer.

  2. Claim 2Depends on #1

    The method of claim 1 further comprising wherein the substrate comprises a high resistivity p-type silicon substrate with a (100) off-cut in the range of about 2 to about 8 degrees towards a direction.

  3. Claim 3Depends on #1

    The method of claim 1 further comprising wherein the GaSb nucleation layer comprises a low melting point material and a thickness of between about 50 angstroms and about 300 angstroms.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗