Method for producing laminated dielectric
Abstract
A method for producing a laminated dielectric, which comprises laminating a raw material layer containing a high dielectric constant glass ceramic composition comprising from 30 to 70 mass % of a Ba—Ti compound powder having a Ti/Ba molar ratio of from 3.0 to 5.7 and from 30 to 70 mass % of an alkali free glass powder containing, by mol %, from 15 to 40% of SiO 2 , from 5 to 37% of B2O3, from 2 to 15% of Al 2 O 3 , from 1 to 25% of CaO+SrO, from 5 to 25% of BaO and from 25 to 50% of SiO 2 +Al 2 O 3 , and a raw material layer containing a low dielectric constant glass ceramic composition comprising from 10 to 70 mass % of a ceramic powder and from 30 to 90 mass % of an alkali free glass powder wherein SiO 2 +Al 2 O 3 is at least 34 mol % and larger by at least 9 mol % than that in the above alkali free glass powder, followed by firing.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 23 · Forward citations: 7.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method for producing a laminated dielectric having a low dielectric constant layer and a high dielectric constant layer alternately laminated in an odd number of layers in total so that a low dielectric constant layer constitutes the outermost layer, which comprises alternately laminating a high dielectric constant raw material layer containing a high dielectric constant glass ceramic composition, to form a high dielectric constant layer having a relative dielectric constant of from 16 to 30 at a frequency of from 1 GHz to 25 GHz, when fired, and a low dielectric constant raw material layer
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (7 of 7 total)
References Cited — Backward Prior Art (23)
Non-Patent Literature (5)
- JP 2003-069236 A (Furuse et al.) Mar. 7, 2003 (English machine translation of foreign patent already of record on applicant's IDS of Jan. 20, 2006). [online] [retrieved Mar. 10, 2009]. Retrieved from: Japan Patent Office Advanced Industrial Property Network.
- Marchand et al., Microstructure of GaN Laterally Overgrown by Metalorganic Chemical Vapor Deposition, Applied Physics Letters, vol. 73, No. 6, Aug. 10, 1998, pp. 747-749.
- Nakamura et al., High-Power, Long-Lifetime InGaN/GaN/AlGaN-Based Laser Diodes Grown on Pure GaN Substrates, Jpn. J. Appl. Phys., vol. 37, Mar. 15, 1998, pp. L309-L312.
- Nakamura et al., InGaN/GaN/AlGaN-Based Laser Diodes Grown on GaN Substrates With a Fundamental Transverse Mode, Jpn. J. Appl. Phys., vol. 37, Sep. 15, 1998. pp. L1020-L1022.
- Nam et al., Lateral Epitaxial Overgrowth of GaN Films on SiO2 Areas Via Metalorganic Vapor Phase Epitaxy, Journal of Electronic Materials, vol. 27, No. 4, 1998, pp. 233-237.