Abstract

A method of forming a semiconductor device that includes heating a wafer on which an Al—Cu sputtering thin film is formed before patterning the Al—Cu sputtering thin film. The heating is performed at a temperature no less than a solid solution temperature of copper or at a temperature between 300° C. and 600° C. The process temperature in heating the process wafer is not higher than the flow temperature of aluminum or is the temperature at which a reflow process can be performed.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 2.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method comprising: forming a partially laminated metal film as a wiring line layer on a wafer; and then heating the wafer including the wiring line layer in a sputtering chamber at a first predetermined temperature after forming the wiring line layer; and then performing a process which completely laminates the wiring line layer on the wafer; and then heating the wafer and the wiring line layer at a second predetermined temperature after completely laminating the wiring line layer on the wafer; and then patterning the completely laminated wiring line layer.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the metal film comprises an aluminum-copper film and the second predetermined temperature is not lower than a solid solution temperature for a copper component in the aluminum-copper film.

  3. Claim 3Depends on #2

    The method of claim 2 , wherein the aluminum-copper film includ