US 7,682,859 B2#6863306 Most CitedActiveUnited States (USPTO)Utility

Patterned strained semiconductor substrate and device

14Forward Citations (#6863306 Global)
0.9/yrCitation Velocity (#8177540 Global)
2.73Citation PageRank (#8799313 Global)
50Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method that includes forming a pattern of strained material and relaxed material on a substrate; forming a strained device in the strained material; and forming a non-strained device in the relaxed material is disclosed. In one embodiment, the strained material is silicon (Si) in either a tensile or compressive state, and the relaxed material is Si in a normal state. A buffer layer of silicon germanium (SiGe), silicon carbon (SiC), or similar material is formed on the substrate and has a lattice constant/structure mis-match with the substrate. A relaxed layer of SiGe, SiC, or similar material is formed on the buffer layer and places the strained material in the tensile or compressive state. In another embodiment, carbon-doped silicon or germanium-doped silicon is used to form the strained material. The structure includes a multi-layered substrate having strained and non-strained materials patterned thereon.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 14.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for forming an electrical device, the method comprising: forming a buffer layer in contact with a portion of a substrate, the buffer layer having a lattice constant/structure mismatch with the substrate; forming a relaxed layer on the buffer layer; forming a strained material on a top surface of the relaxed layer, such that the relaxed layer places the strained material in one of a tensile or a compressive state; forming a strained device in the strained material; and forming a non-strained device directly on the substrate adjacent the strained material.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the relaxed layer comprises a material which has a lattice constant/structure mismatch with the strained material.

  3. Claim 3Depends on #1

    The method of claim 1 , wherein the buffer layer is selected from the group consisting of silicon carbon (SiC), silicon germanium (Si

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • A. Shimizu, et al., "Local Mechanical-Stress Control (LMC): A New Technique for CMOS-Performance Enhancement" International Electron Devices Meeting, IEEE, Mar. 2001.
  • A. Shimizu, et al., "Local Mechanical-Stress Control (LMC): A New Technique for CMOS-Performance Enhancement", International Electron Devices Meeting, IEEE, Mar. 2001.
  • B. Doyle, et al., "Recovery of Hot-Carrier Damage in Reoxidized Nitrided Oxide MOSFETs." IEEE Electron Device Letters, vol. 13, No. 1, Jan. 1992, pp. 38-40.
  • C.J. Huang, et al., "Temperature Dependence and Post-Stress Recovery of Hot Electron Degradation Effects in Bipolar Transistors." IEEE 1991 Bipolar Circuits and Technology Meeting 7.5, pp. 170-173.
  • C.J. Huang, et al., "Temperature Dependence and Post-Stress Recovery of Hot Electron Degradation Effects in Bipolar Transistors." IEEE 1991, Bipolar Circuits and Technology Meeting 7.5, pp. 170-173.