US 7,675,174 B2#77256455 Most CitedExpiredUnited States (USPTO)Utility

Method and structure of a thick metal layer using multiple deposition chambers

0Forward Citations (#77256455 Global)
0.0/yrCitation Velocity (#77256455 Global)
0.56Citation PageRank (#77256455 Global)
34Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A thick metal layer is formed on a semiconductor integrated circuit in multiple different deposition chambers. A first portion of the metal layer is formed in a first deposition chamber, the first thickness being approximately half the target thickness. The substrate is then removed from the first chamber and transported to a second chamber. The deposition of the same metal layer continues in a second chamber, having the same grain structure and orientation. The second portion of the metal layer is grown to achieve the final thickness. By using two different deposition chambers to form the single metal layer, layers in excess of 25,000 angstroms in thickness can be obtained.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 34 · Forward citations: 0.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A semiconductor structure, comprising: a semiconductor substrate having a conductive region therein; a first insulating layer formed over the substrate; a first metal layer formed on top of the first insulating layer; an interconnect structure used to connect the first metal layer to the conductive region of the substrate; a second insulating layer formed on top of the first metal layer; a second metal layer formed on top of the second insulating layer; a third insulating layer formed on top of the second metal layer; a third metal layer formed on top of the third insulating layer; a fourth in

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (34)

PatentTitleYearCitations
JP S57154858 AMethod for formation of electrode—6
US 4,514,265 ABonding pads for semiconductor devices198529
JP S61251153 AFormation of bump of semiconductor device—4
US 4,726,983 AHomogeneous fine grained metal film on substrate and manufacturing method thereof198816
JP H02253628 AManufacture of semiconductor device—11
US 5,060,045 ASemiconductor integrated circuit device and method of manufacturing the same199179
EP 0,465,152 A2Method for producing semiconductor device having alignment mark—8
US 5,108,951 AMethod for forming a metal contact199280
JP H04133330 ASemiconductor device and its connecting method—15
JP H0513421 ABump forming device—13
US 5,298,459 AMethod of manufacturing semiconductor device terminal having a gold bump electrode199441
US 5,310,699 AMethod of manufacturing a bump electrode1994100
EP 0,655,780 A1Method for forming an aluminum contact—19
US 5,447,599 ASelf-aligned process for capping copper lines199545
US 5,470,787 ASemiconductor device solder bump having intrinsic potential for forming an extended eutectic region and method for making and using the same1995218
US 5,587,336 ABump formation on yielded semiconductor dies199643
US 5,773,359 AInterconnect system and method of fabrication1998139
US 5,925,227 AMultichamber sputtering apparatus199973
US 6,130,449 ASemiconductor memory device and a method for fabricating the same2000112
US 6,218,302 B1Method for forming a semiconductor device2001158
US 2001040264 A1Method of forming a semiconductor device and an improved deposition system—13
US 6,329,722 B1Bonding pads for integrated circuits having copper interconnect metallization200188
US 6,476,491 B2Semiconductor device having a multilayer wiring structure and pad electrodes protected from corrosion and method for fabricating the same200256
US 6,504,237 B2Semiconductor with multilayer metal structure using copper that offer high speed performance200316
US 2003038025 A1Method and apparatus for improving sidewall coverage during sputtering in a chamber having an inductively coupled plasma—9
US 6,649,522 B2Etch stop in damascene interconnect structure and method of making200322
US 6,667,552 B1Low dielectric metal silicide lined interconnection system200342
US 6,710,425 B2Structure to increase density of MIM capacitors between adjacent metal layers in an integrated circuit200447
US 6,727,590 B2Semiconductor device with internal bonding pad200490
US 6,747,355 B2Semiconductor device and method for manufacturing the same200446

Non-Patent Literature (5)

  • Hawley, J., et al., "Solutions to Catastrophic Yield Problems in MCM-D Interconnect Production," IEEE, 1998, International Conference on Multichip Modules and High Density Packaging, pp. 118-123.
  • Igarashi et al., "The Best Combination of Aluminum and Copper Interconnects for a High Performance 0.18mum CMOS Logic Device," IEEE: International Electron Devices Meeting, Dec. 6-9, 1998, pp. 31.1.1-31.1.4.
  • Igarashi et al., "The Best Combination of Aluminum and Copper Interconnects for a High Performance 0.18μm CMOS Logic Device," IEEE: International Electron Devices Meeting, Dec. 6-9, 1998, pp. 31.1.1-31.1.4.
  • Pan et al., Integrated Interconnect Module Development, VMIC Conference, Jun. 18-20, 1996, pp. 46-51.
  • Quintana et al., "Thickness Effects on Aluminum Thin Films," Sociedad Mexicana de Ciencia de Superficies y de Vacio, Superficies y Vacio 9, Dec. 1999, pp. 280-282.