Polyanhydride polymers and their uses in biomedical devices
Abstract
A biocompatible, bioerodable polyanhydride polymer having a Young's modulus between about 1.5 and 3 and a selected rate of surface degradation, and methods of forming and using the polymer, are disclosed. The polymer is formed of a polyester prepolymer having a preferred molecular weight of greater than 5 and less than 7.5 Kdaltons, and a selected number of anhydride linkages between 5 and about 30.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 1.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A biodegradable polyester-based polyanhydride polymer having, as a repeating polymer unit, a polylactide, polycaprolactone or polyglycolide α-ω,-dianhydride chain having an average molecular weight greater than 5 and less than 10 Kdaltons, and between 8-12 anhydride linkages, where each anhydride linkage links a pair of adjacent repeating polymer units, and said polymer is characterized by: (i) a Young's modulus between 1.5-3 GPa, and (ii) a rate of surface degradation that is effective to fully erode a bar of the polymer having dimensions of 50 microns×50 microns×2 mm, when incubated in p
- Claim 2Depends on #1
The polymer of claim 1 , wherein the rate of surface degradation is effective to fully erode a bar of the polymer having dimensions of 50 microns×50 microns×2 mm, when incubated in phosphate b
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (1 of 1 total)
References Cited — Backward Prior Art (50)
Non-Patent Literature (5)
- "Therapeutics Company Raises US$9M fro Biodegradable Polymer Stents.", May 10, 1997, The Azo Journal of Materials Online, -www.azom.com/news.asp?newsID=8492 (2007).
- Bryers, J.D. et al., "Biodegradation of poly(anhydride-esters) into non-steroidal anti-inflammatory drugs and their effect on Pseudomonas aeruginosa biofilms in vitro and on the foreign-body response in vivo", Biomaterials, 27(29):5039-5048 (2006).
- Engelberg, I et al., "Physico-mechanical properties of degradable polymers used in medical applications: a comparative study", Biomaterials, 12(3):292-304 (1991).
- Erdmann, L. and Uhrich, K.E., "Synthesis and degradation characteristics of salicylic acid-derived Poly(anhydride-esters)", Biomaterials, 21(19):1941-1946 (2000).
- Erdmann, L. et al., "Degradable poly(anhydride ester) implants: effects of localized salicylic acid release on bone", Biomaterials, 21(24):2507-2512 (2000).