High strain-point glass composition for substrate

4Forward Citations (#25402202 Global)
0.2/yrCitation Velocity (#28513377 Global)
1.31Citation PageRank (#28281975 Global)
9Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

The present invention relates to a glass substrate composition comprising SiO 2 55˜70 wt %, Al 2 O 3 0˜1 wt %, ZrO 2 0.1˜5 wt %, Na 2 O 0.1˜5 wt %, K 2 O 7˜13 wt %, MgO 7˜14 wt %, CaO 0˜4 wt %, SrO 7˜12 wt % and SO 3 0.01˜0.5 wt %. The glass substrate prepared by using the above composition shows less thermal deformation at a baking process under a high temperature since the strain point of the glass is at least 570° C., does not have such disadvantages as increase of fuel cost and short life cycle of refractories resulted from less than 1460° C. of melting point, and has 80˜95×10 −7 /° C. of thermal expansion coefficient in the temperature range of 50˜350° C. Therefore, the glass according to the present invention is suitable as a substrate.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 4.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A glass composition comprising SiO 2 55˜70 wt %, Al 2 O 3 0˜1 wt %, ZrO 2 0.1˜5 wt %, Na 2 O 0.1˜5 wt %, K 2 O 7˜13 wt %, MgO 8˜14 wt %, CaO 0˜less than 1 wt %, SrO 7˜12 wt %, and SO 3 0.01˜0.5 w %, wherein the weight ratio of MgO/CaO is 8 or more.

  2. Claim 2Depends on #1

    The glass composition of claim 1 , wherein the total content of SiO 2 +Al 2 O 3 +ZrO 2 is 60˜72 wt % of the total composition.

  3. Claim 3Depends on #1

    The glass composition of claim 1 , wherein the total content of MgO+CaO+SrO is 15˜24 wt % of the total composition.