Semiconductor device having impurity-doped resistor element
Abstract
Resistor elements are formed by doping impurity into a single crystal film formed on a substrate such as a silicon-on-insulator substrate. A semiconductor device having such resistor elements is used as a detector for detecting an amount of airflow, for example. The impurity density in the single crystal silicon is made lower than 1×10 20 /cm 3 to suppress a resistance change by aging especially at a temperature higher than 310° C. To obtain a high temperature coefficient of the resistor element as well as a low resistance change by aging, the impurity density is set in a range from 4×10 19 /cm 3 to 1×10 20 /cm 3 , and more preferably in a range from 7×10 19 /cm 3 to 1×10 20 /cm 3 . As the impurity, N-type impurity such as phosphorus or P-type impurity such as boron may be used. It is preferable to use the impurity having a low diffusion coefficient to attain a low resistance change by aging.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 16 · Forward citations: 3.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method of manufacturing a semiconductor device, comprising: forming a single crystal silicon film on a substrate via an insulation film; doping impurity into the single crystal silicon film, thereby forming a resistor element, annealing the single crystal film to diffuse the impurity in the single crystal silicon film so that an impurity density is uniform in the single crystal silicon film, wherein the impurity density doped into the single crystal silicon is lower than 1×10 20 /cm 3 and higher than 4×10 19 /cm 3 , and wherein the impurity is phosphorus.
- Claim 2Depends on #1
The method of manufacturing a semiconductor device as in claim 1 , wherein the impurity density is higher than 7×10 19 /cm 3 .
- Claim 3Depends on #1
The method of manufacturing a semiconductor device as in claim 1 , wherein the impurity is N-type impurity having a diffusion coefficient lower than that of p
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (3 of 3 total)
References Cited — Backward Prior Art (16)
Non-Patent Literature (1)
- Notice of Reasons for Rejection mailed on Mar. 17, 2009 issued from the Japanese Patent Office in the corresponding Japanese patent application No. 2007-025940 (and excerpt English translation).