Patents
US 7,670,694 B2#90336715 Most CitedActiveUnited States (USPTO)Utility

Media for recording devices

0Forward Citations (#90336715 Global)
0.0/yrCitation Velocity (#90336715 Global)
0.56Citation PageRank (#90336715 Global)
37Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Improvements to magnetic recording device including magnetic recording media are described. The improvements include the addition of copper to the recording layer as well as improved underlayers. In addition, improved manufacturing processes and magnetic/recording properties for media through heating and oxidation are described.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 37 · Forward citations: 0.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    Recording media for a hard disk drive including: a substrate, an underlayer on the substrate; and a magnetic recording layer including a top magnetic recording layer and a bottom magnetic recording layer on the underlayer wherein: the underlayer includes a CrMoC layer on a CrMoBMn layer on a CrMn layer and the bottom magnetic recording layer includes CoPtCrBCu.

  2. Claim 2Depends on #1

    The recording media of claim 1 , wherein the media is longitudinal.

  3. Claim 3Depends on #1

    The recording media of claim 1 wherein the CrMoC layer includes 1-30 at. % Mo and 1-4 at. % C and has a thickness of 10-100 angstroms.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (37)

PatentTitleYearCitations
US 3,852,098 AMethod for increasing rate of coating using vaporized reactants197466
WO 8,301,945 A1Method of placing a metal oxide film on a surface of a heated glass substrate—6
EP 0,140,513 A1Thin film magnetic recording structures—29
US 4,654,276 AMagnetic recording medium with an underlayer and a cobalt-based magnetic layer198735
US 5,789,056 AThin film magnetic disk with chromium-titanium seed layer199828
US 5,798,142 ACVD method of depositing a silica coating on a heated glass substrate199855
JP H11134631 AMagnetic record medium—4
JP H11250438 AMagnetic recording medium, production of magnetic recording medium and magnetic recorder—4
US 5,993,956 AManganese containing layer for magnetic recording media199956
WO 0,007,954 A1Process for coating glass—6
WO 0,110,789 A1Modified glass surfaces and method of producing the same—3
US 2001036564 A1Magnetic recording medium and manufacturing method thereof—33
US 6,432,563 B1Zinc enhanced hard disk media200230
US 6,593,009 B2Magnetic thin film media with a pre-seed layer of CrTi200311
US 6,599,642 B2High anisotropy alloy for thin film disk20037
JP 2003338027 AMagnetic recording medium—3
US 6,682,834 B2Magnetic storage medium having a high recording density200419
US 6,740,209 B2Multilayer film deposition apparatus, and method and apparatus for manufacturing perpendicular-magnetic-recording media200423
US 6,803,117 B2Magnetic recording medium with an exchange layer structure including a CoCrPtB ferromagnetic layer200421
US 2004214049 A1Magnetic recording medium—14
US 2004253486 A1Magnetic recording media having five element alloy deposited using pulsed direct current sputtering utility—14
US 2004258925 A1Magnetic recording media using directly textured glass—14
US 2004258959 A1Magnetic recording medium and method of forming thereof, and underlayer structure thereof—5
WO 2005/005337 A1Process for chemical vapor deposition of a nitrogen-doped titanium oxide coating—1
US 2005014028 A1Magnetic recording medium, magnetic storage apparatus and recording method—16
US 6,855,439 B1Highly oriented longitudinal magnetic media on direct textured glass substrates20059
US 2005069734 A1Thermally stable low noise magnetic recording media—4
US 2005136291 A1Magnetic recording medium, recording method and magnetic storage apparatus—9
US 2005142389 A1Magnetic recording medium—13
US 6,916,558 B2Magnetic disk using a glass substrate20054

Non-Patent Literature (5)

  • Chen et al., "Effects of Mn- and Zr-Doped CrMo Double Underlayers on Structure and Magnetic Properties . . . ," IEEE Trans. MAG 39, No. 5, pp. 2267-2269, Sep. 2003.
  • Choe et al., "Highly In-Plane Oriented CoCrPtB Longitudinal Media for 130-Gb/ in2 Recording," IEEE Trans. MAG 39, No. 2, pp. 633-638, Mar. 2003.
  • Golan et al., "Vacuum-Deposited Gold Films: I. Factors Affecting the Film Morphology," Surface Sience, vol. 264, Issue 3, pp. 312-326, Mar. 1992.
  • Kawanabe et al., "Cr Migration in CoNiTa/Cr Films by Annealing," IEEE Trans. MAG 26, No. 1, pp. 42-44, Jan. 1990.
  • Lathrop et al., "High Transition Temperature Superconducting Thin Films: In-Situ Growth Process . . . ," Electron Devices Meeting, 1998, Pub. Date Dec. 11-14, 1988, pp. 278-281.