Abstract

A method for spherically granulating and agglomerating metal particles such as tantalum and/or niobium powders is described in the present invention, which includes the steps of: a). comminuting the metal particles to form fine particles having D50 less than 50 μm; b). granulating the comminuted metal particles comprising volatile liquid, for example, tantalum and/or niobium particles comprising volatile liquid, to form wet spherical particles; c). still drying the wet spherical particles and removing volatile liquid to form flowable pre-agglomerated particles with increased bulk density; d). heat treating the pre-agglomerated particles; e). screening the heat treated powder to obtain the flowable agglomerated particles. The present invention provides a flowable spherical agglomerated metal particles, and especially tantalum and/or niobium particles having improved properties. The present agglomerated tantalum powder have a flow rate of at least about 2.0 g/sec, a BET surface area of from about 0.2 to about 6.0 m 2 /g, a FSSS of at least 1.0 μm, a Scott bulk density of from about 1.2 g/cm 3 to about 5.5 g/cm 3 . The present agglomerated niobium powder have a flow rate of at least a

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 14.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for spherically granulating and agglomerating metal particles comprising: (a) comminuting the metal particles to form fine particles having D50 less than about 50 μm; (b) combining the comminuted metal particles with a volatile liquid; (c) granulating the comminuted metal particles combined with the volatile liquid in a granulator to form wet particles; (d) still drying the wet particles and removing the volatile liquid to form flowable pre-agglomerated particles with increased bulk density, wherein said flowable pre-agglomerated particles have a size of less than about 1000 μm and a

  2. Claim 2Independent Claim

    The method

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (14 of 14 total)

PatentTitleYearCitations
US 9,831,041 B2Process for manufacturing agglomerated particles of tantalum, mixed tantalum powder and process for manufacturing same, tantalum pellet and process for manufacturing same, and capacitor20170
CN 107,073,575 ACapacitor anode prepared by a kind of compound tantalum powder and preparation method thereof and the tantalum powder—3
US 10,875,091 B2Metal powder, feedstock, and preparation method therefor20200
US 10,720,283 B2Solid electrolytic capacitor having a high capacitance20200
US 12,151,978 B2Density enhancement methods and compositions20240
US 8,054,611 B2Porous metal thin film, method for manufacturing the same, and capacitor20112
US 10,737,322 B2Composite tantalum powder and process for preparing the same and capacitor anode prepared from the tantalum powder20200
US 2009147446 A1Solid electrolytic capacitor and manufacturing method thereof—3
US 2023395329 A1Method of Producing a Tantalum Capacitor Anode—0
US 2009174987 A1Porous metal thin film, method for manufacturing the same, and capacitor—6
US 8,692,459 B2Organic light-emitting display apparatus and method of manufacturing the organic light-emitting display apparatus20140
US 10,373,764 B2Process for manufacturing agglomerated particles of tantalum, mixed tantalum powder and process for manufacturing same, tantalum pellet and process for manufacturing same, and capacitor20190
US 8,238,078 B2Valve metal particles uniformly containing nitrogen and the method for preparing the same, the valve metal green pellets and sintered pellets, and the electrolytic capacitor anodes20120
US 2009180240 A1Valve metal particles uniformly containing nitrogen and the method for preparing the same, the valve metal green pellets and sintered pellets, and the electrolytic capacitor anodes—6