US 7,659,181 B2#22702462 Most CitedActiveUnited States (USPTO)Utility

Sub-micron space liner and filler process

4Forward Citations (#22702462 Global)
0.2/yrCitation Velocity (#28189710 Global)
2.57Citation PageRank (#9730885 Global)
31Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A method of depositing dielectric material into sub-micron spaces and resultant structures is provided. After a trench is etched in the surface of a wafer, an oxygen barrier is deposited into the trench. An expandable, oxidizable liner, preferably amorphous silicon, is then deposited. The trench is then filled with a spin-on dielectric (SOD) material. A densification process is then applied, whereby the SOD material contracts and the oxidizable liner expands. Preferably, the temperature is ramped up while oxidizing during at least part of the densification process. The resulting trench has a negligible vertical wet etch rate gradient and a negligible recess at the top of the trench.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 31 · Forward citations: 4.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of semiconductor fabrication, the method comprising forming a recess in a substrate; depositing a liner within the recess to define a cavity within the recess; depositing a filler material within the cavity; and contracting the filler material and growing the liner inwardly toward the contracting filler material, including introducing a reactant to the substrate at a temperature between about 200° C. and 600° C., wherein growing the liner comprises oxidizing the liner, contracting comprises curing the filler material in a steam ambient environment in a curing chamber and curing compri

  2. Claim 2Depends on #1

    The method of claim 1 , wherein curing comprises temperature ramping at a rate of between about 3° C. and 25° C. per minute.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (31)

PatentTitleYearCitations
US 4,855,804 AMultilayer trench isolation process and structure198962
US 5,087,586 AProcess for creating fully-recessed field isolation regions by oxidizing a selectively-grown epitaxial silicon layer1992160
US 5,190,889 AMethod of forming trench isolation structure with germanium silicate filling199345
US 5,387,540 AMethod of forming trench isolation structure in an integrated circuit1995105
US 5,447,884 AShallow trench isolation with thin nitride liner1995263
US 5,492,858 AShallow trench isolation process for high aspect ratio trenches1996240
US 5,702,976 AShallow trench isolation using low dielectric constant insulator199788
US 5,869,384 ATrench filling method employing silicon liner layer and gap filling silicon oxide trench fill layer199962
US 5,926,717 AMethod of making an integrated circuit with oxidizable trench liner199941
US 5,943,585 ATrench isolation structure having low K dielectric spacers arranged upon an oxide liner incorporated with nitrogen199992
US 6,027,982 AMethod to form shallow trench isolation structures with improved isolation fill and surface planarity200057
US 6,037,238 AProcess to reduce defect formation occurring during shallow trench isolation formation200090
US 6,046,487 AShallow trench isolation with oxide-nitride/oxynitride liner2000165
US 6,180,490 B1Method of filling shallow trenches2001149
US 6,187,651 B1Methods of forming trench isolation regions using preferred stress relieving layers and techniques to inhibit the occurrence of voids2001123
US 6,316,331 B1Method of making dishing-free insulator in trench isolation200123
US 2002022326 A1Semiconductor device and method of manufacturing the same—55
US 2002064937 A1Methods of manufacturing integrated circuit devices in which a spin on glass insulation layer is dissolved so as to recess the spin on glass insulation layer from the upper surface of a pattern—20
US 6,461,937 B1Methods of forming trench isolation regions having recess-inhibiting layers therein that protect against overetching200274
US 6,500,726 B2Shallow trench isolation type semiconductor device and method of forming the same200240
US 2003022522 A1Method for manufacturing semiconductor device—47
US 6,518,148 B1Method for protecting STI structures with low etching rate liners200344
US 6,576,558 B1High aspect ratio shallow trench using silicon implanted oxide2003105
US 6,657,276 B1Shallow trench isolation (STI) region with high-K liner and method of formation2003148
US 6,699,799 B2Method of forming a semiconductor device200431
US 6,717,231 B2Trench isolation regions having recess-inhibiting layers therein that protect against overetching200443

Non-Patent Literature (3)

  • Advertisement entitled "Polysilazane SODs Spinfir(TM) 400 Series for STI/PMD Application," May 2004.
  • Advertisement entitled "Polysilazane SODs Spinfir™ 400 Series for STI/PMD Application," May 2004.
  • Peters, Laura, "Choices and challenges for shallow trench isolation," Semiconductor International, Website www.ree-electronics.com, Apr. 1, 1999, 6 pages.