Patents
US 7,659,158 B2#3459709 Most CitedActiveUnited States (USPTO)Utility

Atomic layer deposition processes for non-volatile memory devices

23Forward Citations (#3459709 Global)
1.4/yrCitation Velocity (#3754259 Global)
3.44Citation PageRank (#6079392 Global)
50Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

Embodiments of the invention provide memory devices and methods for forming memory devices. In one embodiment, a memory device is provided which includes a floating gate polysilicon layer disposed over source/drain regions of a substrate, a silicon oxynitride layer disposed over the floating gate polysilicon layer, a first aluminum oxide layer disposed over the silicon oxynitride layer, a hafnium silicon oxynitride layer disposed over the first aluminum oxide layer, a second aluminum oxide layer disposed over the hafnium silicon oxynitride layer, and a control gate polysilicon layer disposed over the second aluminum oxide layer. In another embodiment, a memory device is provided which includes a control gate polysilicon layer disposed over an inter-poly dielectric stack disposed over a silicon oxide layer disposed over the floating gate polysilicon layer. The inter-poly dielectric stack contains two silicon oxynitride layers separated by a silicon nitride layer.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 23.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for fabricating a non-volatile memory device, comprising: depositing a floating gate polysilicon layer on a substrate; depositing a silicon oxynitride layer on the floating gate polysilicon layer; depositing a first aluminum oxide layer on the silicon oxynitride layer; depositing a hafnium silicon oxynitride layer on the first aluminum oxide layer; depositing a second aluminum oxide layer on the hafnium silicon oxynitride layer; and depositing a control gate polysilicon layer on the second aluminum oxide layer.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein depositing the silicon oxynitride layer further comprises: depositing a silicon oxide material on the floating gate polysilicon layer; implanting nitrogen into the silicon oxide material a during a plasma nitridation process; and heating the substrate to a temperature of about 700° C. or higher during

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗