Patents
US 7,658,970 B2#61985227 Most CitedActiveUnited States (USPTO)Utility

Noble metal layer formation for copper film deposition

1Forward Citations (#61985227 Global)
0.1/yrCitation Velocity (#53057076 Global)
0.74Citation PageRank (#61985227 Global)
50Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Embodiments described herein relate to depositing a cobalt-containing layer by a cyclical deposition process while forming interconnects on a substrate. In one embodiment, a method for forming an interconnect structure is provided which includes depositing a tungsten-containing barrier layer over an exposed contact metal surface within an aperture formed in an insulating material disposed on a substrate, forming a cobalt-containing layer on the tungsten-containing barrier layer using a cyclical deposition process by sequentially exposing the substrate to a cobalt precursor gas and a silicon reducing gas, wherein the cobalt precursor gas contains a cobalt precursor having a cyclopentadienyl ligand, and depositing a copper material on the cobalt-containing layer.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 1.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for forming an interconnect structure on a substrate surface within a processing chamber, comprising: depositing a tungsten-containing barrier layer over an exposed contact metal surface within an aperture formed in an insulating material disposed on a substrate; forming a cobalt-containing layer on the tungsten-containing barrier layer using a cyclical deposition process by sequentially exposing the substrate to a cobalt precursor gas and a silicon reducing gas, wherein the cobalt precursor gas comprises a cobalt precursor selected from the group consisting of cyclopentadienyl cycloh

  2. Claim 2Independent Claim

    The method of clai

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 5,372,849 AChemical vapor deposition of iron, ruthenium, and osmium1994170
US 5,933,753 AOpen-bottomed via liner structure and method for fabricating same1999256
US 5,962,716 AMethods for preparing ruthenium and osmium compounds199983
US 6,063,705 APrecursor chemistries for chemical vapor deposition of ruthenium and ruthenium oxide2000208
US 6,074,945 AMethods for preparing ruthenium metal films2000142
US 6,114,557 AMethods for preparing ruthenium and osmium compounds200044
US 6,203,613 B1Atomic layer deposition with nitrate containing precursors2001824
JP 2001111000 ASemiconductor element and manufacturing method thereof—104
US 2001006838 A1Methods of forming ruthenium film by changing process conditions during chemical vapor deposition and ruthenium films formed thereby—40
JP 2001237400 AMethod of manufacturing capacitor of semiconductor device—23
US 6,294,836 B1Semiconductor chip interconnect barrier material and fabrication method200184
US 2001054730 A1Metal-insulator-metal capacitor and manufacturing method thereof—60
US 2002000587 A1Method for forming capacitor of nonvolatile semiconductor memory device and the capacitor—26
US 2002004293 A1Method of growing electrical conductors—137
US 6,338,991 B1Semiconductor device and method for manufacturing the same200262
US 6,346,477 B1Method of interlayer mediated epitaxy of cobalt silicide from low temperature chemical vapor deposition of cobalt2002147
US 2002025627 A1RuSixOy-containing adhesion layers and process for fabricating the same—29
US 2002028556 A1RuSixOy-containing adhesion layers and process for fabricating the same—25
US 6,365,502 B1Microelectronic interconnect material with adhesion promotion layer and fabrication method2002111
US 6,372,598 B2Method of forming selective metal layer and method of forming capacitor and filling contact hole using the same2002118
US 2002074577 A1RuSixOy-containing adhesion layers and process for fabricating the same—17
US 2002076881 A1RuSixOy-containing adhesion layers and process for fabricating the same—17
US 2002076837 A1Thin films for magnetic device—99
US 2002081381 A1Atomic layer deposition of cobalt from cobalt metallorganic compounds—93
US 6,423,619 B1Transistor metal gate structure that minimizes non-planarity effects and method of formation200273
US 2002102838 A1Microelectronic interconnect material with adhesion promotion layer and fabrication method—37
US 2002102810 A1Method for fabricating a semiconductor device—44
US 6,440,495 B1Chemical vapor deposition of ruthenium films for metal electrode applications2002127
US 2002121697 A1Process for the formation of RuSixOy-containing barrier layers for high-k dielectrics—26

Non-Patent Literature (5)

  • Aaltonen "Atomic Layer Deposition of Noble Metal Thin Films," Academic Dissertation presented at the Department of Chemistry of the University of Helsinki on Apr. 8, 2005, Helsinki, Finland, pp. 1-71.
  • Aaltonen, et al. "Atomic Layer Deposition of Ruthenium from RuCp2 and Oxygen: Film Growth and Reaction Mechanism Studies," Electrochemical Society Proceedings, vol. 2003-08, pp. 946-953.
  • Aaltonen, et al. "Atomic Layer Deposition of Ruthenium Thin Films from Ru(thd)3 and Oxygen," Chem. Vap. Deposition (2004), 10, No. 4, pp. 215-219.
  • Aaltonen, et al. "Ruthenium Thin Films Grown by Atomic Layer Deposition," Chem. Vap. Deposition (2003), 9, No. 1, pp. 45-49.
  • Aoyama, et al. "Ruthenium Films Prepared by Liquid Source Chemical Vapor Deposition Using Bis-(ethylcyclopentadienyl)ruthenium," Jpn. J. Appl. Phys. vol. 38 (1999), pp. L1134-L1136.