Deicer compositions including corrosion inhibitors for galvanized metal
Abstract
A deicing composition with a carboxylate salt as the primary deicer and that has a low corrosivity to galvanized steel is disclosed. The composition includes a soluble silicate as a corrosion inhibitor and a gluconate salt as a silicate stabilizer to maintain adequate solubility of the silicate salt at pH values below about 11.5.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 17 · Forward citations: 6.
Claims (3 — 2 Independent, 1 Dependent)
- Claim 1Independent Claim
A deicing composition comprising a water solution of: a carboxylate salt of a concentration of from about 30-75% by weight; a corrosion inhibitor comprising a soluble silicate salt; and a gluconate salt, wherein the soluble silicate salt is of a concentration sufficient to limit the corrosion rate of galvanized steel in contact with the solution to no more than about 10 mils per year, and wherein the gluconate salt is of a concentration of about 7-15% by weight and is sufficient to prevent precipitation of the silicate, and wherein the pH of the water solution is about 11.5 or lower.
- Claim 2Depends on #1
The deicing composition of claim 1 , wherein the carboxylate salt is selected from the group consisting of sodium, potassium, calcium, magnesium, and ammonium salts of formate, acetate, propionate or lactate, and combinations thereof.
- Claim 3Independent Claim
The deicing