Patents
US 7,652,090 B2#5398896 Most CitedExpiredUnited States (USPTO)Utility

Fire-resistant silicone polymer compositions

17Forward Citations (#5398896 Global)
1.1/yrCitation Velocity (#6061200 Global)
2.54Citation PageRank (#9898258 Global)
50Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A fire resistant composition comprising: a silicone polymer; mica in an amount of from 5% to 30% by weight based on the total weight of the composition; and a limited amount of glass additive sufficient to enable the formation of a self supporting ceramic material at temperatures above the decomposition temperature of the silicone polymer and below the fire rating temperature of the composition. The glass additive addition required to produce the self supporting ceramic material has been found to be preferably from 0.3% to 8% by weight based on the total weight of the composition. The composition is applicable to products formed for fire wall linings, fire partitions, screens, ceilings or linings, structural fire protection, fire door inserts, window or door seals, intumescent seals, in electrical switchboard cabinets or cables. In one cable application, the composition may be used as the extruded intermediate material ( 2 ) between the conductor ( 3 ) and extruded sheath ( 4 ).

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 17.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A fire resistant polymer composition based on a crosslinkable organopolysiloxane and containing inorganic filler for forming a self supporting ceramic under fire conditions, the composition comprising: the crosslinkable organopolysiloxane present in an amount of from 56.5% to 76.75% by weight of the total composition; mica in an amount of from 5% to 30% by weight based on the total weight of the composition; and a glass additive in a form selected from a group consisting of glass frits, glass fibre, and mixtures thereof in an amount of from 0.3% to 8% by weight based on the total weight of the

  2. Claim 2Depends on #1

    The composition according to claim 1 , wherein the glass additive has a softening point

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • Certified English-language translation of JP-55078073 provided by Schreiber Translation, Inc. Translation made in Oct. 2008.
  • Derwent Abstract Accession No. 01217 B/01, JP 78044397 A (Fujikura Cable Works KK) Nov. 28, 1978 Abstract.
  • Derwent Abstract Accession No. 2001-176528/18, JP 2001035267 A (Yazaki Corp) Feb. 9, 2001 Abstract.
  • Derwent Abstract Accession No. 24284 A/13, JP 53-016758 A (Nitto Electric Ind KK) Feb. 16, 1978 Abstract.
  • Derwent Abstract Accession No. 97-199290/18, JP 09055125 A (Fujikura Ltd) Feb. 25, 1997 Abstract.