High-strength, high-conductivity copper alloy wire excellent in resistance to stress relaxation
Abstract
A high-strength, high conductivity copper alloy wire that is excellent in resistance to stress relaxation, which contains 1.0 to 4.5% by mass of Ni, 0.2 to 1.1% by mass of Si, 0.05 to 1.5% by mass of Sn, and less than 0.005% (including zero) by mass of S, with the balance being Cu and inevitable impurities, wherein the wire has a conductivity of from 20% to 60% IACS and a tensile strength of from 700 to 1,300 MPa, and a method of producing the same.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 2.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
0 to 4.5% by mass of Ni, 0.2 to 1.1% by mass of Si, 0.05 to 1.5% by mass of Sn, and less than 0.005% (including zero) by mass of S, optionally 0.2 to 1.5% by mass of Zn, and optionally one or plural elements selected from the group consisting of 0.005 to 0.3% by mass of Ag, 0.01 to 0.5% by mass of Mn, 0.01 to 0.2% by mass of Mg, 0.005 to 0.2% by mass of Fe, 0.005 to 0.2% by mass of Cr, 0.05 to 2% by mass of Co, and 0.005 to 0.1% by mass of P in a total amount of 0.005 to 2% by mass, with the balance being Cu and inevitable impurities, to form a wire rod; subjecting the wire rod to a solution t
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (2 of 2 total)
References Cited — Backward Prior Art (8)
Non-Patent Literature (2)
- German Office Action issued in corresponding Application No. 103 92 428.0-24 dated Oct. 31, 2006.
- International Search Report issued by Japanese Patent Office on Jun. 17, 2003.