US 7,648,599 B2#5948337 Most CitedExpiredUnited States (USPTO)Utility

Method of preparing nickel titanium alloy for use in manufacturing instruments with improved fatigue resistance

16Forward Citations (#5948337 Global)
1.0/yrCitation Velocity (#6551280 Global)
1.94Citation PageRank (#15225702 Global)
22Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method of treating Nitinol to train the structure thereof to remain in the martensite state, including the steps of subjecting the Nitinol to a strain and while subjected to the strain, thermally cycling the Nitinol between a cold bath of about 0° C. to 10° C. and a hot bath of about 100° C. to 180° C. for a minimum of about five cycles.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 22 · Forward citations: 16.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of treating nickel titanium drawn wire to train the structure thereof to resist cyclic fatigue comprising the steps of: subjecting the wire to elongational strain of between 1% to 10% to stabilize the atomic structure thereof; and while subjected to said elongational strain, thermally cycling the wire between cold and hot baths for a minimum of about three cycles, wherein the cold bath is at about 0° C. to 10° C. and the hot bath is at about 100° C. to 180° C.

  2. Claim 2Depends on #1

    A method according to claim 1 wherein the cold bath employs water sprayed on the wire.

  3. Claim 3Depends on #1

    A method according to claim 1 wherein the hot bath employs a pool of water within which the wire travels.