Patents
US 7,645,694 B2#27391219 Most CitedActiveUnited States (USPTO)Utility

Development or removal of block copolymer or PMMA-b-S-based resist using polar supercritical solvent

4Forward Citations (#27391219 Global)
0.2/yrCitation Velocity (#29016713 Global)
1.00Citation PageRank (#41611189 Global)
45Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Methods of developing or removing a select region of block copolymer films using a polar supercritical solvent to dissolve a select portion are disclosed. In one embodiment, the polar supercritical solvent includes chlorodifluoromethane, which may be exposed to the block copolymer film using supercritical carbon dioxide (CO 2 ) as a carrier or chlorodiflouromethane itself in supercritical form. The invention also includes a method of forming a nano-structure including exposing a polymeric film to a polar supercritical solvent to develop at least a portion of the polymeric film. The invention also includes a method of removing a poly(methyl methacrylate-b-styrene) (PMMA-b-S) based resist using a polar supercritical solvent.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 45 · Forward citations: 4.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of forming a nano-structure, the method comprising the steps of: forming a polymeric film over a substrate; annealing the polymeric film to allow for phase separation of immiscible components; and exposing the polymeric film to a polar supercritical solvent to develop at least a portion of the polymeric film into the nano-structure.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the exposing step includes using supercritical carbon dioxide (CO 2 ) as a carrier for the polar supercritical solvent.

  3. Claim 3Depends on #1

    The method of claim 1 , wherein the exposing step includes exposing in an environment at a temperature of no less than approximately 31° C. and no greater than approximately 80° C., and a pressure of no less than approximately 200 bar and no greater than approximately 300 bar.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (45)

PatentTitleYearCitations
US 4,820,752 AProcess for incorporating an additive into a polymer and product produced thereby198940
US 5,236,602 ADense fluid photochemical process for liquid substrate treatment199395
US 5,665,527 AProcess for generating negative tone resist images utilizing carbon dioxide critical fluid1997106
US 5,688,879 AMethod of making fluoropolymers199717
US 5,908,510 AResidue removal by supercritical fluids1999156
US 5,976,264 ARemoval of fluorine or chlorine residue by liquid CO2199997
US 6,277,753 B1Removal of CMP residue from semiconductors using supercritical carbon dioxide process200194
US 6,306,564 B1Removal of resist or residue from semiconductors using supercritical carbon dioxide2001169
US 6,331,487 B2Removal of polishing residue from substrate using supercritical fluid process200153
US 6,339,121 B1Compatibilizer for immiscible polymer blends200256
US 2002012884 A1Method for patterning a radiation sensitive layer—13
US 6,346,484 B1Method for selective extraction of sacrificial place-holding material used in fabrication of air gap-containing interconnect structures200271
US 6,358,673 B1Pattern formation method and apparatus200242
US 6,379,874 B1Using block copolymers as supercritical fluid developable photoresists200263
US 6,398,875 B1Process of drying semiconductor wafers using liquid or supercritical carbon dioxide200249
US 6,425,956 B1Process for removing chemical mechanical polishing residual slurry200225
US 6,451,375 B1Process for depositing a film on a nanometer structure200221
US 6,454,869 B1Process of cleaning semiconductor processing, handling and manufacturing equipment200220
US 6,500,605 B1Removal of photoresist and residue from substrate using supercritical carbon dioxide process200290
US 6,509,141 B2Removal of photoresist and photoresist residue from semiconductors using supercritical carbon dioxide process200341
US 6,509,136 B1Process of drying a cast polymeric film disposed on a workpiece20036
US 6,521,466 B1Apparatus and method for semiconductor wafer test yield enhancement200329
US 2003047533 A1Method for removing a sacrificial material with a compressed fluid—65
US 6,558,475 B1Process for cleaning a workpiece using supercritical carbon dioxide200351
US 6,561,220 B2Apparatus and method for increasing throughput in fluid processing200312
US 6,562,146 B1Processes for cleaning and drying microelectronic structures using liquid or supercritical carbon dioxide200370

Non-Patent Literature (5)

  • Black, C. T., et al., "High-Capacity, Self-Assembled Metal-Oxide-Semiconductor Decoupling Capacitors," IEEE Electron Device Letters, Jun. 2004, pp. 1-3.
  • Black, C. T., et al., "Integration of Self-Assembled Diblock Copolymers for Semiconductor Capacitor Fabrication," Applied Physics Letters, vol. 79, No. 3, Jul. 2001, pp. 409-411.
  • Guarini, K. W., et al., "Nanoscale Patterning Using Self-Assembled Polymers for Semiconductor Applications," Journal of Vacuum Science Technology B, vol. 19, No. 6, Nov./Dec. 2001, pp. 2784-2788.
  • Schäffer, E. et al., "Electrically Induced Structure Formation and Pattern Transfer," Macmillan Magazines Ltd., Letters to Nature, vol. 403, Feb. 24, 2000, pp. 874-877.
  • Thurn-Albrecht, T., et al., "Ultrahigh-Density Nanowire Arrays Grown in Self-Assembled Diblock Copolymer Templates," Science Magazine, vol. 290, Dec. 15, 2000, pp. 2126-2129.