Bonding method, device produced by this method, and bonding device
Abstract
Conventional heat bonding and anodic bonding require heating at high temperature and for a long time, leading to poor production efficiency and occurrence of a warp due to a difference in thermal expansion, resulting in a defective device. Such a problem is solved. An upper wafer 7 made of glass and a lower wafer 8 made of Si are surface-activated using an energy wave before performing anodic bonding, thereby performing bonding at low temperature and increasing a bonding strength. In addition, preliminary bonding due to surface activation is performed before main bonding due to anodic bonding is performed in a separate step or device, thereby increasing production efficiency, and enabling bonding of a three-layer structure without occurrence of a warp.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 10.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A bonding method which comprises performing anodic bonding of objects to be bonded after subjecting bonding surfaces of both the objects to be bonded to a surface activation treatment using a plasma, wherein the surface activation treatment causes OH groups to covalently adhere to the bonding surfaces, wherein the anodic bonding of the objects causes H 2 O to be released and covalent bonds to be formed between the bonding surfaces, and wherein both the objects to be bonded are heated at less than 400° C. during or after bonding.
- Claim 2Depends on #1
The bonding method according to claim 1 , wherein both the objects to be bonded are heated at less than 400° C. to form the covalent bonds between the bonding surface.
- Claim 3Depends on #1
The bonding method according to claim 1 , wherein after said surface activation treatment, the anodic bonding of both the objects to be bonded is
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗