US 7,638,709 B2#13641693 Most CitedActiveUnited States (USPTO)Utility

Fluoropolymer wire insulation

8Forward Citations (#13641693 Global)
0.5/yrCitation Velocity (#17611686 Global)
1.69Citation PageRank (#18992768 Global)
23Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

FEP compositions are provided that provide foam insulation in coaxial cable that surpasses the return loss obtained when PFA is used to make the foamed insulation, one composition comprising a blend of tetrafluoroethylene/hexafluoropropylene copolymers, one of said copolymers exhibiting a strip force of at least about 3 lbf (13.3 N) and another of said copolymers exhibiting a strip force no greater than about 2.5 lbf (11.1 N), said blend exhibiting a strip force of at least about 3 lbf (13.3 N), each said strip force being the force necessary to break adhesion between conductor and said one of said copolymers, said another of said copolymers, and said blend, respectively, and another composition comprising tetrafluoroethylene/hexafluoropropylene copolymer having an MFR of no greater than about 16 g/10 min and containing —CF 3 end groups and an effective amount of wire affinity end groups to exhibit a strip force of at least about 3 lbf (13.3 N), said strip force being the force necessary to break adhesion between conductor and said copolymer, the coaxial cable exhibiting an average return loss of no greater than about −26 dB at 800 MHz to 3 GHz and having a void content of about 20

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 23 · Forward citations: 8.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    Coaxial cable comprising a central conductor, a foamed insulation on said central conductor, and an outer conductor over said foamed insulation, said foamed insulation having a void content of about 20 to 65% and an average return loss of no greater than about −26 dB at 800 MHz to 3 GHz, said foamed insulation comprising tetrafluoroethylene/hexafluoropropylene copolymer exhibiting a strip force with respect to said central conductor of at least about 3 lbf (13.3 N).

  2. Claim 2Depends on #1

    The coaxial cable of claim 1 wherein said void content is about 45 to 60%.

  3. Claim 3Depends on #1

    The coaxial cable of claim 1 wherein the thickness of said foamed insulation is at least about 0.020 in (0.5 mm).

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (23)

PatentTitleYearCitations
US 4,029,868 ATetrafluoroethylene terpolymers1977212
US 4,742,122 AMelt-processible tetrafluoroethylene/perfluoroolefin copolymers and processes for preparing them198857
US 4,743,658 AStable tetrafluoroethylene copolymers1988355
US 4,764,538 AFoam nucleation system for fluoropolymers198877
US 4,877,815 ANucleating agents for thermoplastic resins198965
EP 0,684,272 A1Foamable solid compositions based on perfluoropolymers and process for the preparation thereof—11
US 5,543,217 AAmorphous copolymers of tetrafluoroethylene and hexafluoropropylene199632
WO 9,702,301 A1Modified polytetrafluoroethylene fine powder—19
US 5,677,217 AMethod for fabricating a mosfet device, with local channel doping and a titanium silicide gate199726
US 5,677,404 ATetrafluoroethylene terpolymer1997140
US 5,726,214 ASelf-foaming fluoropolymer composition199832
EP 0,423,995 B1Low dissipation-factor fluorocarbon resins and cables prepared therefrom19989
WO 0,242,372 A1Conductive fluoropolymers—7
JP 2002293831 AFluorine-containing olefin polymer particle—37
EP 1,260,526 A1Fluoropolymer and electric wire and cable both coated with the same—19
US 6,541,588 B1Tetrafluoroethylene/hexafluoropropylene copolymers with higher drawability200350
US 6,623,680 B2Tetrafluoroethylene/hexafluoropropylene copolymers with higher drawability20039
US 6,743,508 B2Fep pellet200428
EP 1,462,465 A1Melt-processible thermoplastic fluoropolymers having improved processing characteristics and method of producing the same—7
US 2004242783 A1Fluorine-containing resin composition, method for producing the same, and cable having coating comprising the same—26
US 6,838,545 B2Reaction of fluoropolymer melts200551
WO 2006/009761 A1Insulation for an improved high-speed data transmission cable—3

Non-Patent Literature (1)

  • PCT International Search Report and Written Opinion for International Application No. PCT/US2008/063626 dated Jul. 11, 2008.