US 7,632,349 B2#15934545 Most CitedActiveUnited States (USPTO)Utility

Silicon wafer surface defect evaluation method

7Forward Citations (#15934545 Global)
0.4/yrCitation Velocity (#19586856 Global)
1.46Citation PageRank (#23813423 Global)
29Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

There is provided a silicon wafer surface defect evaluation method capable of readily detecting a region where small crystal defects exist, the evaluation method comprising: a rapid heat treatment step of a silicon wafer from a silicon single-crystal ingot in an atmosphere which can nitride silicon at a temperature elevating speed of 10 to 150° C./second from a room temperature to temperatures between not lower than 1170° C. and less than a silicon melting point, holding the silicon wafer at the processing temperature for 1 to 120 seconds and then cooling the silicon wafer to the room temperature at a temperature lowering speed of 10 to 100° C./second; and a step of using a surface photo voltage method to calculate a minority carrier diffusion length on the wafer surface, thereby detecting a region on the wafer surface in which small COP's which cannot be detected at least by a particle counter exist.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 29 · Forward citations: 7.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for evaluating surface defects of a silicon wafer comprising: a rapid heat treatment step wherein a silicon wafer cut out from a silicon single-crystal ingot is subjected to a heat treatment in an atmosphere which includes at least one of an NH 3 gas, N 2 gas, N 2 O gas, an NO gas, or a mixed gas atmosphere containing these gases with an inert gas, and wherein the temperature is elevated at a speed of 10 to 150° C./second from a room temperature to temperatures between 1170° C. and less than the melting point of silicon, holding the silicon wafer at this processing temperature for 1

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (29)

PatentTitleYearCitations
US 4,181,538 AMethod for making defect-free zone by laser-annealing of doped silicon1980123
US 4,598,249 AMethod using surface photovoltage (SPV) measurements for revealing heavy metal contamination of semiconductor material198642
US 5,272,119 AProcess for contamination removal and minority carrier lifetime improvement in silicon199319
US 5,369,495 ASemiconductor contaminant sensing system and method199432
US 5,581,194 AMethod and apparatus for passive optical characterization of semiconductor substrates subjected to high energy (MEV) ion implantation using high-injection surface photovoltage199638
US 5,742,176 AMethod of measuring a Fe-B concentration of a silicon wafer199816
US 5,742,175 AMethod of evaluating a density of oxygen-precipitation defects in a silicon wafer19985
US 5,773,989 AMeasurement of the mobile ion concentration in the oxide layer of a semiconductor wafer199890
US 5,804,981 AMethod of detecting heavy metal impurities introduced into a silicon wafer during ion implantation199827
WO 9,845,507 A1Low defect density, ideal oxygen precipitating silicon—109
EP 0,898,298 A1Determination of the thickness of a denuded zone in a silicon wafer—2
EP 0,964,443 A2Method for heat treatment of silicon wafer and silicon wafer—12
CN 1,256,723 ALow defect density, ideal oxygen precipitating silicon—13
US 6,197,606 B1Determination of the thickness of a denuded zone in a silicon wafer200118
JP 2001081000 AMethod of evaluating crystal defect in silicon single crystal—32
US 6,254,672 B1Low defect density self-interstitial dominated silicon200155
JP 2001217251 AMethod of heat-treating silicon wafer—17
US 2001025597 A1Low defect density, self-interstitial dominated silicon—10
JP 2001274167 ASilicon semiconductor substrate and its manufacturing method—12
US 2002007779 A1Low defect density, self-interstitial dominated silicon—3
US 6,512,384 B1Method for fast and accurate determination of the minority carrier diffusion length from simultaneously measured surface photovoltages200336
US 6,569,691 B1Measurement of different mobile ion concentrations in the oxide layer of a semiconductor wafer200320
US 2004053516 A1Method for producing silicon wafer and silicon wafer—20

Non-Patent Literature (5)

  • English abstract of JP 2001-081000, Mar. 27, 2001.
  • English language Abstract of JP 2001-217251.
  • English language Abstract of JP 2001-274167.
  • Porrini Et Rossetto, "Influence of thermal history during Czochralski silicon crystal growth on OISF nuclei formation", Material Science and Engineering, vol. B36, 1996, pp. 162-166, XP002531516.
  • Slaoui A et al., "Rapid thermal diffusion of phosphorus into silicon from doped oxide films (solar cell manufacture)", Proceedings of the Photovoltaic Specialists Conference. Las Vegas, Oct. 7-11, 1991, [Proceedings of the Photovoltaic Specialists Conference], New York, IEEE, US, vol. Conf. 22, Oct.