Ultraviolet assisted porogen removal and/or curing processes for forming porous low k dielectrics

17Forward Citations (#5428963 Global)
1.0/yrCitation Velocity (#6420958 Global)
2.35Citation PageRank (#11256639 Global)
14Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

Processes for forming porous low k dielectric materials from low k dielectric films containing a porogen material include exposing the low k dielectric film to ultraviolet radiation. In one embodiment, the film is exposed to broadband ultraviolet radiation of less than 240 nm for a period of time and intensity effective to remove the porogen material. In other embodiments, the low k dielectric film is exposed to a first ultraviolet radiation pattern effective to increase a crosslinking density of the film matrix while maintaining a concentration of the porogen material substantially the same before and after exposure to the first ultraviolet radiation pattern. The low k dielectric film can be then be processed to form a metal interconnect structure therein and subsequently exposed to a second ultraviolet radiation pattern effective to remove the porogen material from the low k dielectrics film and form a porous low k dielectric film.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 17.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A process for forming an electrical interconnect structure, the process comprising, in sequence: depositing a non-porous dielectric material onto a substrate, wherein the non-porous dielectric material consists essentially of a matrix and a porogen material; patterning the non-porous dielectric material and forming a metal interconnect structure; and exposing the non-porous low k dielectric material to an ultraviolet radiation pattern for a period of time effective to remove a portion of the porogen material, wherein the removed portion forms pores within the matrix and forms a porous dielectr

  2. Claim 2Depends on #1

    The process of claim 1 , wherein the porous dielectric material has an elastic modulus greater than or equal to about 2.5 GPa.

  3. Claim 3Independent Claim

    The

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (2)

  • James L. Hedrick et al., Templating Nanoporosity in Thin-Film Dielectric Insulators, Advanced Materials 1998, 10, No. 13, pp. 1049-1053.
  • Jeffrey M. Calvert et al., A New Approach to Ultralow-K Dielectrics, Semiconductor International, Nov. 2003, pp. 56-60.