Patents
US 7,628,871 B2#15851225 Most CitedExpiredUnited States (USPTO)Utility

Bulk metallic glass solder material

7Forward Citations (#15851225 Global)
0.4/yrCitation Velocity (#19583278 Global)
1.51Citation PageRank (#22714502 Global)
28Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

High strength, reliable bulk metallic glass (BMG) solder materials formed from alloys possessing deep eutectics with asymmetric liquidous slopes. BMG solder materials are stronger and have a higher elastic modulus than, and therefore are less likely than crystalline solder materials to damage fragile low k interlayer dielectric (ILD) materials due to thermal stress in materials with different coefficients of thermal expansion (CTE). BMG solder materials may physically, electrically, or thermally couple a feature to another feature, or any combination thereof. For example, in an embodiment of the invention, a BMG solder material may physically and electrically couple an electronic component to a printed circuit board. In another embodiment of the invention, a BMG solder material may physically and thermally couple an integrated heat sink to a semiconductor device. Many embodiments of a BMG solder material are also lead-free, so they comply with lead-free product requirements, while providing a better solution than other lead-free solder materials such as tin-silver-copper.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 28 · Forward citations: 7.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    An article of manufacture, comprising: a substrate; a component; and a bulk metallic glass solder material physically coupling the substrate to the component, wherein the bulk metallic glass solder material has an alloy composition which undergoes glass formation when the solder material is cooled from at or above the melting temperature (T m ) to at or below the glass transition temperature (Tg) at a cooling rate below approximately 10 2 ° C./second, and wherein the bulk metallic glass solder material comprises an alloy including at least one of tin-indium including 45-60 wt. % tin, tin-zinc

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (28)

PatentTitleYearCitations
US 4,222,434 ACeramic sponge heat-exchanger member198081
US 4,377,622 AMethod for producing compacts and cladding from glassy metallic alloy filaments by warm extrusion198317
US 4,621,031 AComposite material bonded by an amorphous metal, and preparation thereof1986194
US 4,710,235 AProcess for preparation of liquid phase bonded amorphous materials198756
US 4,901,904 AMethod of producing brazing metals199037
US 5,232,962 AAdhesive bonding composition with bond line limiting spacer system1993130
JP H07256482 ABrazing method—8
US 5,482,580 AJoining of metals using a bulk amorphous intermediate layer199667
US 6,214,480 B1Article made by joining two members together, and a brazing filler metal200115
TW 436,349 BSolder paste containment device20011
US 6,286,206 B1Heat-resistant electronic systems and circuit boards200151
US 6,442,040 B2Embedded memory assembly20024
US 2003042590 A1Electronic component and process for producing the electronic component—9
US 2003164289 A1Methods of making and using freestanding reactive multilayer foils—71
US 2003168130 A1Lead-free solder powder material, lead-free solder paste and a method for preparing same—23
US 6,623,566 B1Method of selection of alloy compositions for bulk metallic glasses200326
US 6,756,687 B1Interfacial strengthening for electroless nickel immersion gold substrates20047
US 6,809,539 B2Probe card for testing an integrated circuit200432
US 2005084407 A1Titanium group powder metallurgy—54
US 2005110162 A1Electronic component having at least one semiconductor chip and flip-chip contacts, and method for producing the same—29
WO 2007/021492 A1Bulk metallic glass solder—1
US 7,187,068 B2Methods and apparatuses for providing stacked-die devices200749
US 2007080451 A1Intermetallic solder with low melting point—36

Non-Patent Literature (5)

  • Andersson, C , et al., "Comparison of isothermal mechanical fatigue properties of lead-free solder joints and bulk solders", ICEPT (2003), 371-376.
  • Boonrat, Lohwongwatana, et al. "Bulk metallic glasses-alloy compositions survey," U.S. Appl. No. 60/921,805, filed Apr. 4, 2007.
  • C Andersson. et al., "Comparison of Isothermal Mechanical Fatigue Properties of Lead-Free Solder Joints and Bulk Solders," Materials Science and Engineering a Structural Materials: Properties, Microstructure & Processing, Luasanne, CH, vol. 394, No. 1-2, Mar. 15, 2005, pp. 20-27.
  • F. Ochoa et al. Effects of Cooling Rate on the Microstructure and Tensile Behavior of a Sn-3.5wt% Ag solder. Journal of Electronic Materials, vol. 32, No. 12, 2003, p. 1414-1420.
  • H. Jones, A perspective on the development of rapid solidification and nonequilibrium processing and its future. Materials Science and Engineering 2001 A304-306 p. 11-19.