Patents
US 7,625,692 B2#98812675 Most CitedActiveUnited States (USPTO)Utility

Yield and line width performance for liquid polymers and other materials

0Forward Citations (#98812675 Global)
0.0/yrCitation Velocity (#98812675 Global)
0.56Citation PageRank (#98812675 Global)
50Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Systems and methods are described for improved yield and line width performance for liquid polymers and other materials. A method for minimizing precipitation of developing reactant by lowering a sudden change in pH includes: developing at least a portion of a polymer layer on a substrate with an initial charge of a developer fluid; then rinsing the polymer with an additional charge of the developer fluid so as to controllably minimize a subsequent sudden change in pH; and then rinsing the polymer with a charge of another fluid. An apparatus for minimizing fluid impingement force on a polymer layer to be developed on a substrate includes: a nozzle including: a developer manifold adapted to supply a developer fluid; a plurality of developer fluid conduits coupled to the developer manifold; a rinse manifold adapted to supply a rinse fluid; and a plurality of rinse fluid conduits coupled to the developer manifold. The developer manifold and the rinse manifold can be staggered so as to reduce an external width of the nozzle compared to a nominal external width of the nozzle achievable without either intersecting the fluid manifold and the another manifold or staggering the fluid manifo

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 0.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for minimizing precipitation of developing reactant, said method comprising: providing a laminar airflow field in a developer fluid module in which a substrate is located; applying a charge of a developer fluid onto a polymer layer on the substrate; developing at least a portion of the polymer layer with the developer fluid; rinsing said polymer layer with an additional charge of said developer fluid so as to controllably minimize a subsequent sudden change in PH; and then rinsing said polymer layer with a rinse fluid having a fluid chemistry different from the developer fluid.

  2. Claim 2Depends on #1

    The method of claim 1 wherein rinsing said polymer layer with rinse fluid includes rinsing said polymer layer with deionized water dispensed in a fine disbursement.

  3. Claim 3Depends on #1

    The method of claim 1 wherein the developer fluid is applied at a plurality o

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 2,295,522 ABlowpipe head194222
US 2,501,724 AApparatus for thermochemically cutting metal195023
US 2,501,725 AInstrument structure for portable testing voltmeters195072
US 3,204,682 AOxy-gas blowpipe196554
US 3,516,607 ASteam application system197019
US 4,326,553 AMegasonic jet cleaner apparatus1982198
JP S57198457 ADeveloping method for photoresist—10
JP S5888749 ADeveloping device—6
JP S58111318 ADeveloping method—11
JP S597949 ADeveloping method—11
JP S5950440 ADeveloping method of resist film—5
EP 0,110,558 A2Method and apparatus for use in developing resist film—14
US 4,457,259 AApparatus for spraying a liquid on a spinning surface198451
US 4,507,333 ABiphenylene end-capped quinoxaline polymers and their use as insulating coatings for semiconductor devices198512
US 4,564,280 AMethod and apparatus for developing resist film including a movable nozzle arm1986148
US 4,576,903 ADeveloper for positive photoresists198633
US 4,721,252 AHot-melt sputtering apparatus198833
US 4,747,541 ADispensing apparatus198832
US 4,872,417 AMethod of and apparatus for automatically coating a workpiece198974
US 4,938,994 AMethod and apparatus for patch coating printed circuit boards1990179
US 5,094,934 AMethod of developing a high contrast, positive photoresist using a developer containing alkanolamine199213
US 5,094,884 AMethod and apparatus for applying a layer of a fluid material on a semiconductor wafer199268
JP H04124812 AStrip liquid nozzle—10
US 5,127,984 ARapid wafer thinning process199251
JP H0555133 ALiquid supply nozzle—13
US 5,234,161 ACounterflow spray nozzle199312
US 5,252,137 ASystem and method for applying a liquid199345
US D341418 SSupply nozzle for applying liquid resist to a semiconductor wafer199313
JP H0645244 ADevelopment method in ic manufacturing—13
US 5,342,738 AResist film developing method and an apparatus for carrying out the same199427

Non-Patent Literature (5)

  • Final Office Action mailed Oct. 17, 2008 for U.S. Appl. No. 11/604,130, filed Nov. 22, 2006, 8 pgs.
  • First Non-Final Rejection mailed Feb. 25, 2008 for U.S. Appl. No. 11/604,130, filed Nov. 22, 2006, 8 pgs.
  • International Search Report PCT/US99/20115.
  • Ito, Hiroshi et al., "Influence of Acid Generator Structure on T-Top Formation in High Temperature Bake Processes for Environmental Stabilization," SPIE, vol. 2438, pp. 53-59.
  • Laxman, Ravi K., "Low e Dielectrics: CVD Fluorinated Silicon Dioxides," Semiconductor International, May 1995, pp. 71, 74.