Patents
US 7,625,536 B2#33378881 Most CitedExpiredUnited States (USPTO)Utility

Titaniferous ore beneficiation

3Forward Citations (#33378881 Global)
0.2/yrCitation Velocity (#35557042 Global)
1.04Citation PageRank (#39445541 Global)
22Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

This invention relates to a process for beneficiating a titaniferous ore. The process comprises leaching the titaniferous ore with sulfuric acid to form a leached ore, calcining the leached ore in the presence of oxygen to form a calcined ore, and leaching the calcined ore with sulfuric acid, hydrochloric acid, and/or nitric acid to form a beneficiated ore. The leached ore is not reduced prior to or following calcination.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 22 · Forward citations: 3.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A process for beneficiating a naturally occurring anatase titaniferous ore or a naturally occurring anatase titaniferous ore body comprising a blend of anatase ore with ilmenite ore comprising: (a) leaching the titaniferous ore or the titaniferous ore body with sulfuric acid at a temperature of at least 110° C. to form a leached ore and a liquid phase; (b) calcining the leached ore in the presence of oxygen or in the presence of an oxygen-containing gas at a temperature of greater than 800° C. to form a calcined ore; and (c) leaching the calcined ore with an acid selected from the group consis

  2. Claim 2Depends on #1

    The process of claim 1 wherein the sulfuric acid of step (a) is primarily obtained from a waste stream and/or a recycle stream.

  3. Claim 3Independent Claim

    The proces

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (22)

PatentTitleYearCitations
US 2,811,434 AProcess for treating ilmenite-containing materials to produce metallic iron concentrates and titanium dioxide concentrates195710
US 3,777,013 AProcess for the preparation of synthetic rutile starting from ilmenite19739
US 3,784,670 ATitanium dixide concentrate and its manufacturing process197432
US 4,176,159 AProcess for concentration of titanium containing anatase ore197921
EP 0,243,725 A2Method for purifying titanium oxide ores—18
CA 1,234,990 AProcess of producing an tio.sub.2 concentrate from tio.sub.2-containing starting materials19883
US 5,011,666 AMethod for purifying TiO2 ore199128
WO 9,113,180 A1Production of synthetic rutile—16
US 5,085,837 AMethod for purifying TiO2 ore by alternate leaching with an aqueous solution of an alkali metal compound and an aqueous solution of mineral acid199223
WO 9,220,827 A1METHOD FOR PURIFYING TiO2 ORE—12
US 5,181,956 AMethod for purifying TiO2 ore199318
WO 9,524,510 A1Leaching of titaniferous materials—9
US 5,730,774 AProcess for upgrading titaniferous materials199815
US 5,826,162 Aleaching of titaniferous materials199827
US 5,830,420 AMethod to upgrade titania slag and resulting product199823
US 6,048,505 AContinuous non-polluting liquid phase titanium dioxide process and apparatus200040
US 2001051120 A1Process for the production titanium concentrate having a chemical composition similar to ilmenite from highly impure anatase ores—39
US 2002168310 A1Process for upgrading a titaniferous material containing silica—4
US 2003198591 A1Acid benefication of ore—17
US 6,803,024 B1Benefication of titania slag by oxidation and reduction treatment200411
WO 2005/042405 A1A PROCESS TO OBTAIN TITANIUM CONCENTRATES WITH HIGH CONTENTS OF TiO2 AND LOW CONTENTS OF RADIONUCLIDE ELEMENTS FROM ANATASE MECHANICAL CONCENTRATES—14
US 7,008,602 B2Beneficiation of titaniferous ore with sulfuric acid200610

Non-Patent Literature (1)

  • PCT Search Report dated Jun. 15, 2007.