Method for improved formation of nickel silicide contacts in semiconductor devices
Abstract
A method of forming silicide contacts for semiconductor devices includes subjecting a silicon containing semiconductor wafer to a degas treatment at an initial degas temperature of about 250 to about 400° C., transferring the semiconductor wafer from a degas chamber to a deposition chamber, depositing a nickel containing layer over the wafer following transfer of the wafer from the degas chamber to the deposition chamber, and annealing the semiconductor wafer so as to create silicide regions at portions on the wafer where nickel material is formed over silicon.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 17 · Forward citations: 1.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A method of forming silicide contacts for semiconductor devices, the method comprising: subjecting a silicon containing semiconductor wafer to a degas treatment at an initial degas temperature of about 400° C.; transferring the semiconductor wafer from a degas chamber to a deposition chamber; depositing a nickel containing layer over the wafer following transfer of the wafer from the degas chamber to the deposition chamber, wherein the nickel containing layer is deposited at a point in time when the semiconductor wafer has cooled to temperature range of about 250° C. to less than the initial d
- Claim 2Depends on #1
The method of claim 1 , wherein the wafer is cooled for about 30 seconds to about 5 minutes betwee
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (1 of 1 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 9,312,121 B1 | Method for cleaning contact hole and forming contact plug therein | 2016 | 0 |