Patents
US 7,619,028 B2#23331542 Most CitedExpiredUnited States (USPTO)Utility

Diene rubber composition and process for producing the same

4Forward Citations (#23331542 Global)
0.2/yrCitation Velocity (#30385507 Global)
1.73Citation PageRank (#18368851 Global)
14Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

The present invention is to provide a diene rubber composition and a cross-linked diene rubber thereof excellent in tensile strength, wear resistance and processability, keeping compatibility of both good fuel efficiency and high gripping property, and a production method thereof. What is characterized in the composition is that the composition is comprised of 100 parts by weight of a diene rubber having a molecular weight distribution expressed in terms of the ratio of the weight-average molecular weight to the number-average molecular weight of 1.1 to 30, 20 to 200 parts by weight of silica and a cationic polymer, and that a toluene-insoluble rubber content per gram of the silica within the range from 0.2 to 1 g, and diene cross-linked rubber thereof. What is characterized in the production method is that the method comprises steps of allowing rubber latex stabilized by an anionic emulsifying agent to react with an aqueous suspension of silica containing a cationic polymer and effecting co-coagulation of rubber in the rubber latex with the silica in the aqueous suspension within a specific pH range.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 4.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A diene rubber co-coagulation product obtained by mixing and co-coagulating a diene rubber latex with silica which has been mixed with a cationic polymer, comprising 100 parts by weight of a diene rubber having a molecular weight distribution expressed in terms of a ratio of weight-average molecular weight to number-average molecular weight being 1.1 to 30, 20 to 200 parts by weight of silica and a cationic polymer, wherein a toluene-insoluble rubber content per gram of the silica is within the range from 0.2 to 1 g.

  2. Claim 2Depends on #1

    The diene rubber co-coagulation product as set forth in claim 1 , wherein the specific surface area of the silica (unit: m 2 /g) measured by the adsorption method using cetyl trimethyl ammonium bromide (CTAB) is 60 to 300 m 2 /g.

  3. Claim 3Depends on #1

    The diene rubber co-coagulation product as set forth in claim 1 , wherein 0.1 to 7.5 parts by we

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (2)

  • JP 2001-213971 (Aug. 2001) abstract and translation in English.
  • JP 2003-221402 (Aug. 2003) abstract and translation in English.