Patents
US 7,618,706 B2#8673937 Most CitedExpiredUnited States (USPTO)Utility

Process for making high-performance polyethylene multifilament yarn

12Forward Citations (#8673937 Global)
0.7/yrCitation Velocity (#10700521 Global)
1.70Citation PageRank (#18787134 Global)
13Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

The invention relates to a process for making high-performance polyethylene multi-filament yarn comprising the steps of a) making a solution of ultra-high molar mass polyethylene in a solvent; b) spinning of the solution through a spinplate containing at least 5 spinholes into an air-gap to form fluid filaments, while applying a draw ratio DRfluid; c) cooling the fluid filaments to form solvent-containing gel filaments; d) removing at least partly the solvent from the filaments; and e) drawing the filaments in at least one step before, during and/or after said solvent removing, while applying a draw ratio DRsolid of at least 4, wherein in step b) each spinhole comprises a contraction zone of specific dimension and a downstream zone of diameter Dn and length Dn with Ln/Dn of from 0 to at most 25, to result in a draw ratio DRfluid=DRsp*DRag of at least 150, wherein DRsp is the draw ratio in the spinholes and DRag is the draw ratio in the air-gap, with DRsp being greater than 1 and DRag at least 1. The invention further relates to a high-performance polyethylene multifilament yarn, and to semi-finished or end-use products containing said yarn, especially to ropes and ballistic-resista

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 12.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    High-performance polyethylene multifilament yarn comprising n filaments and having a tensile strength of at least f *(n −0.065 ) GPa, wherein factor f is at least 5.8 and n is at least 5, and wherein the filaments are made from linear ultra-high molar mass polyethylene of IV 8-40 dl/g as measured on solutions in decalin at 135° C.

  2. Claim 2Depends on #1

    High-performance polyethylene multifilament yarn according to claim 1 wherein f has a value from 6.0 to 10.

  3. Claim 3Depends on #1

    High-performance polyethylene multifilament yarn according to claim 1 , showing a non-reversible peak, as measured by temperature-modulated differential scanning calorimetry, with a maximum at about 152° C. and having an enthalpy of at least 35 J/g.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (2)

  • International Search Report.
  • Patent Abstract of Japan, vol. 005, No. 128, Aug. 18, 1981 & JP 56 063004 A, May 29, 1981.