Cerium-based oxide fiber and its fabricating method
Abstract
This invention discloses a kind of cerium-based oxide fiber and its fabricating method. The cerium-based hydrate fiber can be synthesized by aging under the boiling point of water for 10 hours to 50 hours by the addition of a chemical modifier. The fibers show a diameter of submicron to micron size, and the aspect ratio is greater than 100. The hydrate fibers can transform to oxide fiber after calcination at high temperature.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 2.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A cerium-based fiber fabrication method, comprising the steps of: adding a modifier, cerium nitrate, sodium hydroxide, and metal (M1, M2) nitrate into an a solution according to a predetermined ratio (h) of sodium hydroxide to cerium nitrate and a predetermined ratio of M1, M2 to cerium nitrate, wherein said modifier is a citric acid or a citric acid derivative compound; waiting till solutes of said solution are dissolved completely; placing said solution into a constant temperature machine for holding the temperature; and removing said solution and a produced precipitate in several hours afte
- Claim 2Depends on #1
The fabrication method of claim 1 , wherein said sodium hydroxide and said citric acid have a ratio (h), and 0.25<h<0.7.
- Claim 3Depends on #1
The fabrication method of claim 1