Positive electrode active material for non-aqueous electrolyte secondary battery and manufacturing method thereof, and non-aqueous electrolyte secondary battery using same
Abstract
To provide a positive electrode active material for a non-aqueous electrolyte secondary battery, which if used as a positive electrode for a lithium ion secondary battery, the battery internal resistance can be reduced, giving a secondary battery superior in output characteristics and life property. After mixing raw material powders in specified quantities of each so as to become a lithium-metal complex oxide represented by LizNi1-wMwO2 (wherein M is at least one kind or more of metal elements selected from the group consisting of Co, Al, Mg, Mn, Ti, Fe, Cu, Zn, and Ga; and w and z respectively satisfy 0<w<=0.25, and 1.0<=z<=1.1), baking is performed in two stages. At first the temperature is raised from room temperature to a first stage baking temperature (450 to 550° C.) at a temperature rise rate of 0.5 and 15° C./min, and held for 1 to 10 hours. Then the temperature is raised to a second stage baking temperature (650 to 800° C.), and held for 0.6 to 30 hours.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 4.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A positive electrode active material for a non-aqueous electrolyte secondary battery comprising: primary particles of a lithium-metal complex oxide powder which is a lithium-metal complex oxide powder represented by Li z Ni 1-w M w O 2 , wherein M is at least one metal element selected from the group consisting of Co, Al, Mg, Mn, Ti, Fe, Cu, Zn, and Ga; and w and z respectively satisfy 0<w≦0.25, and 1.0≦z≦1.1; and secondary particles which are formed by aggregating a plurality of the primary particles, wherein: the shape of the secondary particles is spherical or spheroidal; 95% or more of