Patents
US 7,601,631 B2#21860071 Most CitedActiveUnited States (USPTO)Utility

Very low dielectric constant plasma-enhanced CVD films

5Forward Citations (#21860071 Global)
0.3/yrCitation Velocity (#26307489 Global)
1.31Citation PageRank (#28206408 Global)
50Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

The present invention provides a method for depositing nano-porous low dielectric constant films by reacting an oxidizable silicon containing compound or mixture comprising an oxidizable silicon component and an oxidizable non-silicon component having thermally liable groups with nitrous oxide, oxygen, ozone, or other source of reactive oxygen in gas-phase plasma-enhanced reaction. The deposited silicon oxide based film is annealed to form dispersed microscopic voids that remain in a nano-porous silicon oxide based film having a low-density structure. The nano-porous silicon oxide based films are useful for forming layers between metal lines with or without liner or cap layers. The nano-porous silicon oxide based films may also be used as an intermetal dielectric layer for fabricating dual damascene structures. Preferred nano-porous silicon oxide based films are produced by reaction of methylsilyl-1,4-dioxinyl ether or methylsiloxanyl furan and 2,4,6-trisilaoxane or cyclo-1,3,5,7-tetrasilylene-2,6-dioxy-4,8 dimethylene with nitrous oxide or oxygen followed by a cure/anneal that includes a gradual increase in temperature.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 5.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for depositing a porous dielectric layer, comprising: depositing a dielectric layer comprising a dispersed organic compound at a temperature less than about 50° C., wherein the dispersed organic compound comprises thermally labile organic groups attached to the dielectric layer; and annealing the dielectric layer, wherein the annealing comprises raising the temperature by about 50° C./minute to a final temperature between about 350° C. to about 450° C.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the annealing converts the dispersed organic compound to dispersed voids.

  3. Claim 3Depends on #1

    The method of claim 1 , wherein the dielectric layer is annealed for five minutes.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 4,610,859 AProcess for producing silicon hydrides198648
US 4,845,054 ALow temperature chemical vapor deposition of silicon dioxide films1989146
US 4,933,430 AProcess for producing polymers useful in thermoset coatings and polymer so produced199013
US 5,010,166 AProcess and apparatus for producing polyol polymers and polyol polymers so produced1991139
US 5,028,566 AMethod of forming silicon dioxide glass films1991116
EP 0,522,799 A2Dielectric deposition—44
EP 0,528,540 A2Thin-film coatings made by means of plasma-activated chemical vapor deposition of fluorinated cyclic siloxanes—22
US 5,312,503 ALaminated magnetic core and method of manufacturing same199410
US 5,314,724 AProcess for forming silicon oxide film1994371
US 5,420,132 ASubstituted benzodioxins199519
EP 0,703,611 A1Method for insulating metal leads using a low dielectric constant material, and structures formed therewith—19
US 5,508,234 AMicrocavity structures, fabrication processes, and applications thereof199662
US 5,541,022 AComposite anode for nonaqueous secondary battery and method for producing the same199659
US 5,540,132 AMethod and apparatus for teaching musical notation to young children199658
US 5,638,251 ACapacitive thin films using diamond-like nanocomposite materials1997141
US 5,741,626 AMethod for forming a dielectric tantalum nitride layer as an anti-reflective coating (ARC)1998316
US 5,776,990 AFoamed polymer for use as dielectric material1998177
US 5,849,644 ASemiconductor processing methods of chemical vapor depositing SiO2 on a substrate199831
GB 2,326,765 AMultilayer wiring—14
WO 9,915,711 A1Laminate comprising a barrier layer of silicon oxide—16
US 5,918,146 AMethod of manufacturing semiconductor device having multilayer wiring structure, with improved version of step of forming interlayer dielectric layer199923
EP 0,935,283 A2Silicone polymer insulation film on semiconductor substrate and method for forming the film—47
WO 9,941,423 A2Plasma processes for depositing low dielectric constant films—169
US 5,989,998 AMethod of forming interlayer insulating film1999213
US 5,990,015 ADual damascence process199959

Non-Patent Literature (5)

  • Australian Examination Report for SG 200006722-3, dated Nov. 12, 2003.
  • Australian Search Report for SG 200006722-3, dated Nov. 1, 2002.
  • European Partial Search Report for EP 00 12 6111.4-1235, dated Sep. 24, 2004.
  • European Search Report for EP 00 12 6111.4-1235, dated Apr. 5, 2005.
  • Kumar, "Dielectric Properties of Plasma Polymerized Furan Thin Film Capacitors" Material Letter, vol. 41 (1999) pp. 1-4.