A high-strength steel pipe excellent in weldability on site and a method for producing the steel pipe by improving the reliability of the low temperature toughness of a steel are provided. For example, the steel pipe includes elements to enhance hardenability for furthering high-strengthening and also improving toughness at a weld heat affected zone subjected to double or more layer welding. In the method, the steel is made to consist of a structure composed of bainite and/or martensite by containing prescribed amounts of C, Si, Mn, P, S, Ni, Mo, Nb, Ti, Al and N, and, as occasion demands, one or more of B, V, Cu, Cr, Ca, REM, and Mg, and regulating C, Si, Mn, Cr, Ni, Cu, V and Mo. Such elements enhancing hardenability, by a specific relational expression. The diameter of prior austenite grains may be regulated in a prescribed range. The method may include heating a casting to a temperature not lower than the Ac3 point, hot rolling such casting, and thereafter cooling the resulting hot-rolled steel plate at a prescribed cooling rate.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 25 · Forward citations: 5.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A high-strength steel pipe having a high low temperature toughness reliability and a high weld heat-affected zone toughness, comprising: a seam-welded portion having multiple layers obtained by applying multi-layer welding, wherein the portion is at least twice heated; and a base steel portion containing, in mass: C: 0.02 to 0.07%, Si: not more than 0.6%, Mn: 1.5 to 2.5%, P: not more than 0.015%, S: not more than 0.003%, Ni: 0.01 to 2.0%, Mo: 0.1 to 0.8%, Nb: 0.001% to 0.005% Ti: 0.005% to 0.030%, B: 0.0003 to 0.0030%, Al: not more than 0.070%, and N: not more than 0.0060%, so as to satisfy th

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (25)

PatentTitleYearCitations
JP S5873717 AProduction of low temperature steel—5
JP S58153730 AMethod of manufacturing high-tensile strength steel plate for use at low temperature—5
JP H03136130 ABatch job applying system by command procedure—1
US 5,134,267 AMethod of conducting circumferential welding of electric welded steel line pipe to be laid by reel barge199212
US 5,454,883 AHigh toughness low yield ratio, high fatigue strength steel plate and process of producing same1995124
JP H08209290 AHigh tensile strength steel for welding excellent in low temperature toughness—8
JP H093545 AProduction of large diameter welded steel tube—7
EP 0,757,113 A1High-strength line-pipe steel having low yield ratio and excellent low-temperature toughness—57
JP H0941080 AWeldability high strength steel having low yield ratio and excellent in low temperature toughness—9
JP H0949025 AProduction of uoe steel pipe excellent in collapsing resistance—22
JP H101744 ASteel excellent in toughness at weld heat-affected zone—2
US 5,798,004 AWeldable high strength steel having excellent low temperature toughness199842
EP 0,861,915 A1High-toughness, high-tensile-strength steel and method of manufacturing the same—26
WO 9,905,336 A1Ultra-high strength, weldable, boron-containing steels with superior toughness—16
JP H1136042 AHigh tensile strength steel excellent in arrestability and weldability and its production—33
JP H11172365 AHigh tensile strength steel excellent in characteristic in center part and its production—18
JP H11229078 AHigh tensile strength steel plate excellent in toughness of parent metal and large heat-input weld heat affected zone and its production—9
JP 2000119749 AProduction of chromium-molybdenum seamless steel pipe for machine structure—9
JP 2000199036 ASuperhigh strength linepipe excellent in low temperature toughness and its production—14
US 6,183,573 B1High-toughness, high-tensile-strength steel and method of manufacturing the same200123
US 6,188,037 B1Welded high-strength steel structures and method of manufacturing the same200146
JP 2001303191 AUltrahigh strength steel pipe for line pipe, excellent in haz toughness in weld zone, and its manufacturing method—15
JP 2001340990 ATube stock of high strength thick-walled welded bend steel tube having superior toughness at welded portion—6
JP 2003136130 AMethod for manufacturing inner and outer surface submerged arc welded steel pipe excellent in toughness characteristics of seam welded portion—12
US 7,018,488 B2Steel pipe for use in reinforcement of automobile and method for production thereof20068

Non-Patent Literature (2)

  • Patent abstract of Japanese Publication No. 09165620 published Jun. 24, 1997.
  • Patent abstract of Japanese Publication No. 09165621 published Jun. 24, 1997.