Patents
US 7,598,320 B2#38449450 Most CitedExpiredUnited States (USPTO)Utility

Protected polyvinyl alcohol auxiliary for forming fine pattern and process for producing the same

2Forward Citations (#38449450 Global)
0.1/yrCitation Velocity (#43202112 Global)
1.06Citation PageRank (#38475236 Global)
50Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A modified polyvinyl alcohol (PVA) protected with a protecting group of the present invention is one wherein an amount of high-molecular weight body components of the modified polyvinyl alcohol having a weight-average molecular weight of 250,000 or more as determined by polyethylene glycol standards according to a gel permeation chromatography is 1000 ppm or less in the modified polyvinyl alcohol. The modified PVA is prepared by removing a metal ion and an acid from the modified PVA such as acetalized PVA with ion exchange treatment and then heat-treating at 80° C. or higher. An auxiliary for fine pattern formation of the present invention comprises the aforementioned modified PVA, a water-soluble crosslinking agent, and water or a mixed solvent of water and a water-soluble organic solvent. The auxiliary for fine pattern formation is applied over a resist pattern 3 and a coated layer 4 is formed thereon. Then the resist pattern 3 and the coated layer 4 are heated and thereby an acid is diffused from the resist pattern 3 to the coated layer 4 . As a result, the coated layer in the vicinity of the resist pattern surface is crosslinked and cured by the diffused acid. The coated layer

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 2.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    An auxiliary for fine pattern formation comprising a modified polyvinyl alcohol protected with a protecting group, a water-soluble crosslinking agent, and water or a mixed solvent of water and a water-soluble organic solvent, wherein the amount of high-molecular weight body components of the modified polyvinyl alcohol protected with a protecting group, which has a weight-average molecular weight of 250,000 or more as determined by polyethylene glycol standards according to a gel permeation chromatography, is 1000 ppm or less in the modified polyvinyl alcohol.

  2. Claim 2Depends on #1

    The auxiliary for fine pattern formation according to claim 1 , wherein the modified polyvinyl alcohol protected with a protecting group is one that was treated so as to remove acid components and metal ions therefrom.

  3. Claim 3Depends on #1

    The auxiliary of claim 1 , where the protecting group is selecte

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (2 of 2 total)

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 3,104,205 ADeodorant composition comprising the copper complex of the copolymer of allylamine and methacrylic acid196348
US 3,666,473 APositive photoresists for projection exposure1972110
JP S51125154 AA process for preparing polyvinyl alcohol with a limited distribution of molecular weight—6
JP S51125155 AA process for preparing polyvinyl alcohol with a narrow distribution o f molecular weight—5
JP S61173376 AKeyboard device for word processor—4
EP 0,250,248 A2Block copolymer, method of making the same, diamine precursors of the same method, method of making such diamines and end products comprising the block copolymer—96
JP S63278911 AManufacture of ultra-low-molecular weight polyvinyl alcohol—10
US 4,812,551 ANovolak resin for positive photoresist198956
US 4,823,345 AMethod and apparatus for communication network alert record identification198984
JP H01221750 APattern forming or correcting method—6
US 5,035,881 ADentifrice composition199118
JP H03200805 APurification of water-soluble polyvinyl acetal—15
JP H05241348 APattern forming method—51
US 5,294,444 ATransparent or semi-transparent cosmetic composition199432
JP H0681173 AFormation of metallic film pattern—6
JP H06250379 APattern forming method and formation of photomask for phase shift method—57
US 5,538,820 AReticulation resistant photoresist coating199617
US 5,547,812 AComposition for eliminating microbridging in chemically amplified photoresists comprising a polymer blend of a poly(hydroxystyrene) and a copolymer made of hydroxystyrene and an acrylic monomer199623
WO 9,634,029 A1Polydiorganosiloxane polyurea segmented copolymers and a process for making same—75
US 5,585,219 AResist composition and process for forming resist pattern199696
JP H09235318 AN-allylurethane-based polymer and its production—7
JP H09244262 AAqueous developer for photosensitive printing plate—8
WO 9,740,103 A1Silicone compositions containing a silicone-urea segmented copolymer—89
JP H09325502 ADeveloping method of photosensitive resin composition—10
JP H1073927 AFine pattern forming material, manufacture of semiconductor device using same, and semiconductor device—162
JP H10120968 AResin composition for resist protection film, resist protection film and pattern producing method using the film—19
JP H10158328 AProduction of polyvinyl acetal resin—8
US 5,777,060 ASilicon-containing biocompatible membranes1998149

Non-Patent Literature (5)

  • English Derwent Abstract AN 1996-497582 [49] corres. to DE 696 23456 T2.
  • English Derwent Abstract AN2003-268185 [26], corres. to DE 101 37 855 A1.
  • English Derwent Abstract AN2003-312878 [30] corres. to WO 03/018704 A1.
  • English Language Abstract of JP 10-120968 A, May 12, 1998.
  • English Language Abstract of JP 10-158328 A, Jun. 16, 1998.