Patents
US 7,597,757 B2#14664589 Most CitedExpiredUnited States (USPTO)Utility

ZnO film with C-axis orientation

7Forward Citations (#14664589 Global)
0.4/yrCitation Velocity (#19519355 Global)
2.13Citation PageRank (#13177435 Global)
1Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A ZnO film with a C-axis preference is provided with a corresponding fabrication method. The method includes: forming a substrate; forming an amorphous Al 2 O 3 film overlying the substrate; and, forming a ZnO film overlying the Al 2 O 3 film at a substrate temperature of about 170° C., having a C-axis preference responsive to the adjacent Al 2 O 3 film. The substrate can be a material such as Silicon (Si) (100), Si (111), Si (110), quartz, glass, plastic, or zirconia. The Al 2 O 3 film can be deposited using a chemical vapor deposition (CVD), atomic layer deposition (ALD), or sputtering process. Typically, the Al 2 O 3 layer has a thickness in the range of about 3 to 15 nanometers (nm). The step of forming the ZnO film having a C-axis preference typically means that the ZnO film has a (002) peak at least 5 times greater than the (100) peak, as measured by X-ray diffraction (XRD).

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 1 · Forward citations: 7.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for fabricating a ZnO film with a C-axis preference, the method comprising: forming a substrate; forming an amorphous Al 2 O 3 film overlying the substrate; forming a ZnO film overlying the Al 2 O 3 film from an ALD process using diethylzinc (DEZ) and water, at a substrate temperature of about 170° C., having a C-axis preference responsive to the presence of the Al 2 O 3 film; subsequent to forming the ZnO film, annealing the ZnO film at a temperature in the range of about 400 to 900° C.; and, in response to the annealing, increasing the ZnO film C-axis preference.

  2. Claim 2Depends on #1

    The method of claim 1 wherein forming the substrate includes forming a substrate from a material selected from the group consisting of Silicon (Si) (100), Si (111), Si (110), quartz, glass, plastic, and zirconia.

  3. Claim 3Depends on #1

    The method of claim 1 wherein forming the amorphous

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (1)

Non-Patent Literature (1)

  • Hu et al., "Preparation of piezoelectric coefficient modulated multilayer film ZnO/AI2O3 and its ultrahigh frequency resonance", Applied Physics Letters 71(4) Jul. 28, 1997 p. 548-50.