Method of manufacturing a complementary metal oxide silicon image sensor
Abstract
A method for manufacturing a CMOS image sensor increases the performance of the CMOS image sensor by reducing a peeling phenomenon near a wafer edge and a preventing a circle defect in a pixel region. The method reduces defects in the external appearance of the pad. In order to accomplish the object, there is provided a method for manufacturing a CMOS image sensor, the method including depositing an oxide layer and a nitride layer after forming a pad on a substrate. The pad is exposed and cleaned by etching the oxide layer and the nitride layer. A portion of the oxide layer and the nitride layer over the edge region of the substrate may be etched and removed. A first ashing process, a solvent cleaning process, and a second ashing process may be performed. A pad protection layer is deposited. A hydrogen anneal process is performed. A micro-lens process, a planarization process, and a color filter array process are performed. The pad protection layer over a pad area is removed.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 2.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A method of manufacturing a CMOS image sensor comprising: forming a pad over a substrate; depositing an oxide layer and a nitride layer over the substrate; exposing and cleaning the pad by etching the oxide layer and the nitride layer, wherein said cleaning includes a first ashing process, a solvent cleaning process and a second ashing process; depositing a pad protection layer; performing a hydrogen anneal process; performing a micro-lens process, a planarization process, and a color filter array process; and removing the pad protection layer over a pad area, wherein said exposing and cleanin
- Claim 2Depends on #1
The method of claim 1 , wherein ashing time of the second ashing step is greater t