US 7,592,381 B2#43376022 Most CitedActiveUnited States (USPTO)Utility

Process for preparing a bituminous binder composition

2Forward Citations (#43376022 Global)
0.1/yrCitation Velocity (#43320712 Global)
0.93Citation PageRank (#45886150 Global)
50Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The present invention is directed to a process for preparing a polymer modified bituminous binder composition in the substantial absence of crosslinking agents by heating a bitumen component in a stirred tank to a temperature from 185° C. to 221° C.; adding a block copolymer composition to the bitumen component while the bitumen component is being stirred to form a homogeneous mixture of the bitumen component and the block copolymer composition; and continuing to stir the homogeneous mixture while maintaining the temperature from 185° C. to 221° C. for a period of time from 4 hours to 30 hours thereby forming a cured polymer modified bituminous binder composition. The block copolymer composition utilized in the process comprises a diblock copolymer comprising one block of a monovinylaromatic hydrocarbon and one block of a conjugated diene having a peak molecular weight from 30,000 to 78,000 and a vinyl content from 35 to 80 mol percent based on the number of repeat monomer units in the conjugated diene block, and optionally one or more block copolymers comprising at least two blocks of monovinylaromatic hydrocarbon and at least one block of conjugated diene, the block copolymer sel

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 2.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for preparing a polymer modified bituminous binder composition in the substantial absence of crosslinking agents, said process comprising the steps of: a. heating a bitumen component in a stirred tank to a temperature from 185° C. to 221° C.; b. adding a block copolymer composition to the bitumen component while the bitumen component is being stirred to form a homogeneous mixture of the bitumen component and the block copolymer composition; and c. continuing to stir the homogeneous mixture while maintaining the temperature from 185° C. to 221° C. for a period of time from 4 hours to

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 3,231,635 AProcess for the preparation of block copolymers1966201
US 3,244,664 ASilicon-containing polymers1966195
US 3,251,905 AMethod of preparing block copolymers of conjugated dienes and vinyl-substituted aromatic compounds using dilithio catalysts and diluent mixture of hydrocarbon and ether1966183
US 3,281,383 ABranched polymers prepared from monolithium-terminated polymers and compounds having at least three reactive sites1966316
US 3,390,207 AMethod of making block copolymers of dienes and vinyl aryl compounds1968125
US 3,594,452 APolymers prepared from monolithiumterminated block copolymers and certain diesters1971150
US 3,598,887 APreparation of block copolymers1971123
US 3,692,874 AProcess of coupling alkali metal-terminated polymers with silicic compound in presence of conjugated dienes197298
US 3,880,954 AMethoxy silane coupling of block copolymer formed in cyclohexane197550
US 3,985,830 AStar polymers and process for the preparation thereof1976256
US 4,076,915 ATreatment of coupled polymers prior to hydrogenation197834
US 4,104,332 ACoupling of alkali metal-terminated polymers197855
US 4,129,541 AAsphaltic compositions containing conjugated diene-monovinyl-substituted aromatic hydrocarbon copolymers of particular structures197835
US 4,145,322 AProcess for preparing bitumen-polymer compositions1979143
US 4,185,042 ACoupling agent1980138
US 4,219,627 AProcess for the preparation of block copolymers1980119
US 4,242,246 AProcess for the preparation of bituminous compositions making use of a mother solution containing polymers and sulfur1980107
US 4,379,891 AMultifunctional coupling agent198351
US 4,412,019 AAsphalt compositions198353
US 4,530,652 AAsphalt composition198559
JP S63234063 AAsphalt composition—7
EP 0,413,294 A2Narrow molecular weight distribution block polymers and process therefor—37
JP H03143961 AAsphalt composition with excellent heat resistance—10
JP H03281515 AProduction of new linear block copolymer—6
JP H03281651 AAsphalt composition—9
JP H03287617 AProduction of linear block copolymer—7
US 5,075,377 ABlock copolymer composition1991102
US 5,182,319 APressure sensitive bituminous compositions199319