Aluminum nitride sintered body, method of manufacturing aluminum nitride sintered body, and member
Abstract
An aluminum nitride sintered body is provided, wherein an average crystal grain diameter is 2.0 μm or less, a crystalline phase detected by an X-ray diffractometer is an AlN phase only or an AlN phase and an AlON phase only, and SiO 2 or MgO is present in an amount of more than 0.05 wt % to less than 1 wt %.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 0.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
An aluminum nitride sintered body, wherein an average crystal grain diameter is 2.0 μm or less, a crystalline phase detected by an X-ray diffractometer is an AlN phase only or an AlN phase and an AlON phase only, and SiO 2 or MgO is contained in an amount of more than 0.05 wt % to less than 1 wt %.
- Claim 2Depends on #1
The method of manufacturing the aluminum nitride sintered body according to claim 1 , wherein the aluminum nitride sintered body is manufactured by sintering an aluminum nitride powder in a temperature range of more than 1600° C. to less than 1750° C.
- Claim 3Depends on #2
The method of manufacturing the aluminum nitride sintered body according to claim 2 , wherein an average crystal grain diameter of the aluminum nitride powder is within a range of 0.5 μm to 1.0 μm.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.