Patents
US 7,586,571 B2#21417148 Most CitedExpiredUnited States (USPTO)Utility

Composite double refraction member

5Forward Citations (#21417148 Global)
0.3/yrCitation Velocity (#26252798 Global)
1.39Citation PageRank (#25763338 Global)
21Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The present invention provides a composite birefringent member including a first birefringent layer and a second birefringent layer. The second birefringent layer is formed on at least one surface of the first birefringent layer. In the wavelength range from 400 to 800 nm, a value of Δnd x /Δnd 550 and a value of Rth x /Rth 550 of the composite birefringent member as a whole are different from each other. The composite birefringent member satisfies a requirement that the second birefringent layer is formed of a polymer such as polyamide and/or a requirement that Δnd and Rth of the composite birefringent member satisfy formulae (I) and (II) below. As a result, the composite birefringent member allows a liquid crystal display to achieve a wide viewing angle, compensates birefringence of a liquid crystal cell, and does not cause display coloring of the liquid crystal display. Δ nd 400 /Δnd 550 <1 (I) Rth 400 /Rth 550 >1 (II).

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 21 · Forward citations: 5.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A composite birefringent member comprising: a first birefringent layer; and a second birefringent layer, the second birefringent layer being formed on at least one surface of the first birefringent layer, wherein a value of Δnd x /Δnd 550 and a value of Rth x /Rth 550 of the composite birefringent member as a whole are different from each other in a wavelength range from 400 to 800 nm except 550 nm, and the composite birefringent member satisfies at least one of the following requirements (a) and (b): (a) the second birefringent layer is formed of at least one non-liquid crystal polymer sele

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (21)

PatentTitleYearCitations
JP H0324502 APhase difference plate—30
JP H0333719 ALiquid crystal display device—27
EP 0,487,359 A2A liquid crystal display—8
JP H04194820 ALiquid crystal display device—14
WO 9,424,191 A1Negative birefringent polyimide films—24
WO 9,611,967 A1Negative birefringent rigid rod polymer films—19
JP H08511812 A負複屈折のポリイミド膜—31
WO 9,744,704 A1Polyimide angularity enhancement layer—25
JP H10508048 A負の複屈折性リジッドロッド重合体フィルム—28
JP 2000227520 APhase difference plate, laminated polarizing plate and liquid crystal display device—59
JP 2000511296 Aポリイミド広角化層—33
JP 2001049110 ALow dielectric resin composition—29
US 6,238,753 B1Polyimide angularity enhancement layer200120
EP 1,160,591 A1Transparent film—56
US 6,330,108 B1Composite retarder plate, optically compensatory polarizing plate and liquid-crystal display device200176
JP 2001343529 AProtective film for polarizer and its manufacturing method—145
JP 2002277635 ALaminated retardation plate, polarizing plate and liquid crystal panel using them—7
US 2003086033 A1Laminated phase retarder, polarizing member and liquid-crystal display device—31
WO 03,071,319 A1Stacked phase shift sheet, stacked polarizing plate including the same and image display—7
WO 2004/068226 A1Bi-axial retardation compensation film and vertically aligned liquid crystal display using the same—33
US 2005099562 A1Stacked phase shift sheet, stacked polarizing plate including the same and image display—49

Non-Patent Literature (1)

  • Office Action of Corresponding Taiwanese Patent Application No. 93125803 issued Oct. 9, 2007.