US 7,585,704 B2#11305129 Most CitedExpiredUnited States (USPTO)Utility

Method of producing highly strained PECVD silicon nitride thin films at low temperature

9Forward Citations (#11305129 Global)
0.5/yrCitation Velocity (#14885921 Global)
2.51Citation PageRank (#10111294 Global)
22Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method for increasing the level of stress for amorphous thin film stressors by means of modifying the internal structure of such stressors is provided. The method includes first forming a first portion of an amorphous film stressor material on at least a surface of a substrate, said first portion having a first state of mechanical strain defining a first stress value. After the forming step, the first portion of the amorphous film stressor material is densified such that the first state of mechanical strain is not substantially altered, while increasing the first stress value. In some embodiments, the steps of forming and densifying are repeated any number of times to obtain a preselected and desired thickness for the stressor.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 22 · Forward citations: 9.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of increasing the stress level of an as deposited stressor material comprising: forming an amorphous film stressor material on at least a surface of a substrate, said amorphous film stressor material having a tensile mechanical strain defining a stress value, and is selected from a hydrogen-containing nitride, a hydrogen-containing oxide, or a hydrogen-containing metal; and densifying the amorphous film stressor material such that the state of mechanical strain is not substantially altered, while increasing the stress value, said densifying forms an upper region having a thickness fro

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (22)

PatentTitleYearCitations
US 4,742,020 AMultilayering process for stress accommodation in deposited polysilicon198862
US 4,794,064 AAmorphous silicon electrophotographic receptor having controlled carbon and boron contents198815
US 4,859,554 AMultilayer photoreceptor19896
US 5,153,701 ASemiconductor device with low defect density oxide199228
US 5,720,642 AManufacture of electron emitter utilizing reaction film199814
US 5,756,404 ATwo-step nitride deposition199842
US 5,976,637 AMethod for coating heterogeneous substrates with homogeneous layers19992
US 5,981,403 ALayered silicon nitride deposition process199921
US 6,134,971 AStress induced voltage fluctuation for measuring stress and strain in materials200020
US 2003040158 A1Semiconductor device and method of fabricating the same—247
US 2004071890 A1Method for producing electrophotographic photosensitive member, electrophotographic photosensitive member and electrophotographic apparatus using the same—4
US 2004075148 A1Semiconductor device—156
US 2005253173 A1Dual work-function metal gates—21
US 2005269650 A1Semiconductor device having stress and its manufacture method—61
US 7,022,561 B2CMOS device200665
US 2006157795 A1Structure and method to optimize strain in cmosfets—28
US 7,105,394 B2Semiconductor device and a method of manufacturing the same200685
US 7,125,758 B2Controlling the properties and uniformity of a silicon nitride film by controlling the film forming precursors200633
US 2007023843 A1Semiconductor device and a method of manufacturing the same—9
US 2007102768 A1Semiconductor device and a method of manufacturing the same—11
US 7,262,472 B2Semiconductor device having stress and its manufacture method200716

Non-Patent Literature (1)

  • Growth Study of Wide Bandgap a-Si:H and a-SiN:H by PECVD Method for application in thin film transistor, Jasruddi et al., ICSE 2000 Proceedings, Nov. 2000.