Stable aqueous suspension liquid of finely divided diamond particles, metallic film containing diamond particles and method of producing the same
Abstract
An aqueous suspension liquid of finely divided diamond particles comprising 0.05 to 160 parts by weight of a finely divided diamond particles in 1000 parts of water, wherein; (i) the finely divided diamond particles have an element composition consisting mainly of 72 to 89.5% by weight of carbon, 0.8 to 1.5% of hydrogen, 1.5 to 2.5% of nitrogen, and 10.5 to 25.0% of oxygen; (ii) and, almost all of said diamond particles are in the range of 2 nm to 50 nm in diameters thereof (80% or more by number average, 70% or more by weight average), (iii) and, said finely divided diamond particles exhibit a strongest peak of the intensity of the Bragg angle at 43.9° (2theta±2°), strong and characteristic peaks at 73.5° (2theta±2°)and 95° (2theta±2°), a warped halo at 17° (2theta±2°), and no peak at 26.5°, by X-ray diffraction (XRD) spectrum analysis using Cu-Kalpha radiation when dried, (iv) and, specific surface area of said diamond particles when dry state powder is not smaller than 1.50x105 m2/kg, and substantially all the surface carbon atoms of said particles are bonded with hetero atoms, and the total absorption space of said powder is 0.5 m3/kg or more, when dried. The diamond particles
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 18 · Forward citations: 4.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A metal plating solution comprising diamond powder dispersed and suspended therein at a concentration of 0.01 to 160 g per liter, wherein; (i) said diamond powder have an element composition consisting mainly of carbon in the range of 72 to 89.5% by weight, hydrogen in the range of 0.8 to 1.5%, nitrogen in the range of 1.5 to 2.5% of, and oxygen in the range of 10.5 to 25.0%, (ii) and, 80% or more by number average and/or 70% or more by weight average of particles of said diamond powder are in the range of 2 nm to 50 nm in diameters thereof, (iii) and, said particles of said powder exhibit a s
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (4 of 4 total)
References Cited — Backward Prior Art (18)
Non-Patent Literature (5)
- A. E. Aleksenski{hacek over (i)}, et al.; Effect of Hydrogen on the Structure of Ultradisperse Diamond; Physics of the Solid State, 2000, vol. 42, No. 8, pp. 1575-1578.
- Chen et al. "Spherical nanometer-sized diamond obtained from detonation", Diamond and Related Materials 9 (2000) 1722-1725.
- Dolmatov V. Yu, et al; Industrial Synthesis of Detonation Nanodiamonds and the Technologies on Their Basis.
- Dolmatov V. Yu, et al; New Generation of Metal-Diamond Galvanic Coatings on the Basis of Detonation Synthesis Nanodiamonds.
- K. Iakoubovskii, et al.; Structure and defects of detonation synthesis nanodiamond; Diamond and Related Materials, 2000, vol. 9, pp. 861-865.