Method for cleaning a semiconductor wafer
Abstract
Bottom electrodes of stacked capacitor DRAM cells are formed by depositing a metal layer on the side walls of trenches within a hard mask layer, which serves as a mold for the bottom electrode elements. Prior to depositing the hard mask layer a sacrificial first metal layer is disposed, which results in an electrically conductive surface on the semiconductor wafer. The mask layer is wet-etched to release the bottom electrode as free standing elements on the semiconductor surface. Using the conductive path provided by the first and the second metal layers, the bottom electrodes are polarized in a cleaning liquid bath during a wafer drying process. The generated repulsive electric field overcomes the attractive forces between the neighboring bottom electrode elements induced due to capillary effects of the liquids used for etching and cleaning.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 21 · Forward citations: 0.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method for cleaning a semiconductor wafer having a plurality of metallic structures protruding from a surface of the semiconductor wafer, the method comprising: forming an electrically conductive layer on the surface of the semiconductor wafer, the conductive layer electrically coupling the metallic structures to each other; immersing the semiconductor wafer into a cleaning liquid; polarizing the electrically conductive layer; and withdrawing the semiconductor wafer from the cleaning liquid into a drying atmosphere.
- Claim 2Depends on #1
The method of claim 1 , wherein the polarization of the electrically conductive layer provides a repulsive electrical force between protrusions of the metallic structure.
- Claim 3Depends on #1
The method of claim 1 , wherein the electrically conductive layer is formed from portions of the metallic structures disposed along the surface o
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (21)
Non-Patent Literature (3)
- C. H. Mastrangelo, "Mechanical Stability and Adhesion of Microstructures Under Capillary Forces-Part I: Basic Theory," Journal of Microelectromechanical Systems, vol. 2, No. 1, Mar. 1993, pp. 33-43.
- C. H. Mastrangelo, "Suppression of Stiction in MEMS," 1999 Spring MRS Meeting, Boston, MA, 1999, pp. 1-12.
- Jung-Mu Kim et al., "Continuous Anti-Stiction Coatings Using Self-Assembled Monolayers for Gold Microstructures," Journal of Micromechanics and Microengineering, 12 (2002) pp. 688-695.