Abstract
A chamber dry cleaning process particularly useful after a dielectric plasma etch process which exposes an underlying copper metallization. After the dielectric etch process, the production wafer is removed from the chamber and a cleaning gas is excited into a plasma to clean the chamber walls and recover the dielectric etching characteristic of the chamber. Preferably, the cleaning gas is reducing such as hydrogen gas with the addition of nitrogen gas. Alternatively, the cleaning gas may an oxidizing gas. If the wafer pedestal is vacant during the cleaning, it is not electrically biased. If a dummy wafer is placed on the pedestal during cleaning, the pedestal is biased. The cleaning process is advantageously performed every wafer cycle.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 3.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A process for etching and chamber cleaning, comprising: (a) inserting into a plasma etch chamber a production substrate from a cassette having one or more production substrates and the production substrate comprises a dielectric layer overlying a metal layer; (b) plasma etching the dielectric layer to expose the metal layer; (c) removing the production substrate from the chamber; (d) cleaning the chamber with a plasma of a reducing cleaning gas consisting essentially of a mixture of nitrogen gas and hydrogen gas; (e) then cleaning the chamber with a plasma of a gas consisting essentially of ox
- Claim 2Depends on #1
The process of claim 1 , wherein a bottom portion of the dielectric layer comprises silicon carbide.
- Claim 3Depends on #1
The process of claim 1 , wherein the metal layer co