Patents
US 7,572,865 B2#21849065 Most CitedExpiredUnited States (USPTO)Utility

Polyester films

5Forward Citations (#21849065 Global)
0.3/yrCitation Velocity (#26306199 Global)
1.31Citation PageRank (#28129910 Global)
18Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

The present invention is a polyester film obtained by blending 10-90 wt % of polyester (A) containing ethylene terephthalate as a main constituent component and 90-10 wt % of crystalline polyester (B) different from this polyester (A), which has a half value width of a recrystallization peak obtained by a differential scanning calorimeter (DSC) by lowering temperature of not more than 0.25. The crystalline polyester (B) is preferably a polyester selected from polybutylene terephthalate (PBT), polytrimethylene terephthalate (PTT) and polyethylene 2,6 naphthalate (PEN). According to the polyester of the present invention, a polyester film superior in mechanical characteristic and design property and having high crystallinity, which can be used alone or adhered to a metal sheet and which is free of whitening even when the film is heat treated at near or not lower than the melting point can be obtained, and further, a polyester film having such superior resistance to whitening (design property), which is not easily damaged, can be obtained.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 18 · Forward citations: 5.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A film made from a polyester resin composition comprising 10-90 wt % of polyester (A) comprising ethylene terephthalate as a main constituent component and 90-10 wt % of crystalline polyester (B) different from said polyester (A), which film shows a half value width of recrystallization peak obtained by a differential scanning calorimeter (DSC) by lowering temperature of not more than 0.22; wherein crystalline polyester (B) is a polyester selected from polybutylene terephthalate (PBT) and polytrimethylene terephthalate (PTT).

  2. Claim 2Depends on #1

    The polyester film of claim 1 , wherein a peak temperature (Tc2) of the recrystallization peak is not less than 180° C.

  3. Claim 3Depends on #1

    The polyester film of claim 1 , wherein the polyester film has a reduced viscosity of not less than 0.80.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗