Method for monitoring and calibrating temperature in semiconductor processing chambers

5Forward Citations (#21874414 Global)
0.3/yrCitation Velocity (#26309288 Global)
1.31Citation PageRank (#28294774 Global)
6Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

The present invention provides a non-destructive method for monitoring and calibrating chamber temperature. One embodiment of the present invention provides a method for measuring temperature comprising forming a target film on a test substrate at a first temperature, wherein the target film has one or more properties responsive to thermal exposure, exposing the target film to an environment at a second temperature in a range higher than the first temperature, measuring the one or more properties of the target film after exposing the target film to the environment at the second temperature, and determining the second temperature according to the measured one or more properties.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 5.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for measuring temperature, comprising: forming a target film on a test substrate at a first temperature, wherein the target film has one or more properties responsive to thermal exposure; exposing the target film to an environment at a second temperature in a range higher than the first temperature; measuring the one or more properties of the target film after exposing the target film to the environment at the second temperature; and determining the second temperature according to the measured one or more properties.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the target film is a silicon dioxide (SiO 2 ) film formed by a low temperature atomic layer deposition (ALD).

  3. Claim 3Depends on #2

    The method of claim 2 , wherein forming the target film comprises: exposing the test substrate to a silicon precursor comprising hexachlorodisilane (HCDS); and exposing the te

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • Sneh, et al article, Adsorption and Desorption Kinetics of H2O On A Fully Hydroxylated SiO2 Surface, Dept. of Chemistry and Biochemistry, University of Colorado. Surface Science 364 (1996), pp. 61-78.