Manufacturing method of semiconductor device
Abstract
A manufacturing method of a CMOS semiconductor device includes using, in an nMOS, spike RTA (first annealing) together with ultra-rapid rising/falling temperature annealing (second annealing) whose temperature increase/decrease rate is higher than that of the spike RTA, and applying the ultra-rapid rising/falling temperature annealing (second annealing) alone in a pMOS, when activating a shallow source/drain extension region.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 1.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method of manufacturing a semiconductor device comprising: forming an n-type well and a p-type well on a semiconductor substrate; enclosing upper ends of the n-type well and the p-type well with an isolation film; forming a gate insulating film on the n-type well and the p-type well enclosed with the isolation film; forming gate electrodes on the gate insulating film of the n-type well and the p- type well; forming first sidewall insulating films on the sidewalls of the gate electrodes; forming a first source/drain region and a second source/drain region on upper surfaces of the n-type well
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (1 of 1 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 2011215426 A1 | Semiconductor device and manufacturing method of semiconductor device | — | 1 |