Method of making a glass envelope

4Forward Citations (#25780025 Global)
0.2/yrCitation Velocity (#30536473 Global)
1.27Citation PageRank (#29565884 Global)
19Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

The coefficient of absorption of a pre-selected region of a glass sheet is preferentially increased. The glass sheet may thereafter be sealed to a substrate using a sealing laser. In one embodiment, the coefficient of absorption sheet is increased by irradiating the glass sheet at a wavelength of about 248 nm, preferably through a mask, to produce an irradiated pattern on the glass sheet having a pre-determined shape. The glass sheet is then heat treated, placed over a substrate and sealed to the substrate by exposing the irradiated pattern to a sealing laser light having a wavelength in the range between about 355 nm and 532 nm to produce a glass envelope. The method disclosed herein is useful, inter alia, for manufacturing electro-luminescent devices, such as light emitting diodes (LEDs) and in particular organic light emitting diodes (OLEDs).

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 19 · Forward citations: 4.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for making a glass envelope comprising: providing a first glass sheet having a first side and a second side and doped with Ag or Au; irradiating a portion of the glass sheet with a first optical energy; heating treating the glass sheet at a temperature of at least about 480° C.; positioning the glass sheet over a substrate; and exposing the irradiated portion of the glass sheet to a second optical energy to fuse the glass sheet to the substrate and form a cavity therebetween.

  2. Claim 2Depends on #1

    The method according to claim 1 wherein the first optical energy is at a wavelength of about 248 nm.

  3. Claim 3Depends on #1

    The method according to claim 1 wherein the second optical energy is at a wavelength of between about 300 nm and 600 nm.