Abstract

A method for producing a cobalt on alumina catalyst is disclosed. The catalyst is prepared by thoroughly mixing cobalt nitrate into a peptized alumina slurry, and then spray-drying the slurry to form attrition resistant microspheres. The cobalt prepared by this invention is fully reducible. Optionally, metals such as ruthenium can be added to the cobalt/alumina catalyst by impregnation or methods known in the prior art.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 31 · Forward citations: 10.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for the preparation of an attrition-resistant, cobalt-alumina catalyst comprising the steps: a) preparing an alumina slurry by combining an alumina powder with a peptizing agent, wherein said peptizing agent is selected from the group consisting of an acidic aluminum salt, an acidic cobalt salt, a mineral acid, a carboxy acid, and combinations thereof; b) combining a cobalt source with said alumina slurry; c) allowing said cobalt and alumina slurry to gel; d) homogenizing said cobalt and alumina gel with a sufficient amount of water to form a homogenized slurry; and e) spray-drying sa

  2. Claim 2Depends on #1

    The method of claim 1 further including milling said alumina

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (31)

PatentTitleYearCitations
US 3,361,682 AAlumina-based catalyst and method of preparing same196816
US 3,853,788 AProcess for hydrotreating catalyst and product thereby197416
US 3,980,552 AHydrodesulfurization of residual petroleum oil with a sulfided cobalt-molybdenum-alumina catalyst197615
US 4,016,106 APreparation of catalysts of predetermined pore size distribution and pore volume197750
US 4,082,697 ACatalyst carrier, its method of preparation and a reforming catalyst supported on the carrier197819
US 4,113,661 AMethod for preparing a hydrodesulfurization catalyst197835
US 4,145,316 APreparation of catalysts of predetermined pore size distribution and pore volume197918
US 4,179,411 AMethod of preparing a controlled pore volume alumina with citric acid197929
US 4,623,669 AFischer-Tropsch catalysts19866
JP S6438144 AProduction of catalyst for synthesizing hydrocarbon—4
US 4,831,009 AMethod of applying a catalyst to a support19898
US 4,880,523 AProcess for hydrotreating hydrocarbon feeds19895
US 4,956,516 ADisproportionation of olefins19907
US 5,192,734 AHydroprocessing catalyst composition199328
US 5,302,622 ACobalt-based catalyst and process for converting synthesis gas into hydrocarbons199437
US 5,302,368 AProcess for preparation of alumina199468
US 5,733,839 ACatalysts1998143
US 5,858,325 AAgglomeration of alumina material199912
US 6,043,187 ACatalyst for hydrotreating hydrocarbon feeds in a fixed bed reactor200023
US 6,117,814 ATitania catalysts their preparation and use in fischer-tropsch synthesis200054