Scintillator material and radiation detectors containing same
Abstract
A sintered, annealed scintillator composition, which, prior to annealing, has a formula of A 3 B 2 C 3 O 12 , where A is at least one member of the group consisting of Tb, Ce, and Lu, or combinations thereof, B is an octahedral site (Al), and C is a tetrahedral site (also Al). One or more substitutions are included. The substitutions may may be partial or, in some cases, complete, and can include Al with Sc at B, up to two atoms of oxygen with fluorine and the same number of Ca atoms at A, replacement at B with Mg and the same number of atoms of oxygen with fluorine, replacement at B with a combination of Mg/Si Mg/Zr, Mg/Ti, and/or Mg/Hf, replacement at B with a combination of Li/Nb and/or Li/Ta, and at A with Ca and replacement of an equal number of B or C with silicon.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 7.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A sintered, annealed scintillator composition comprising, prior to annealing: Tb 2.9489 Lu 0.05 Ce 0.0051 Ca 0.005 Al 4.996 O 11.995 F 0.005 .
- Claim 2Depends on #1
A composition in accordance with claim 1 on or essentially adjacent a semiconductor detector matrix so as to form, in combination therewith, an x-ray detector array.
- Claim 3Depends on #1
A composition in accordance with claim 1 , annealed in air at 1200° C. for approximately 24 hours.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗