Semiconductor manufacturing method and semiconductor laser device manufacturing method

2Forward Citations (#42952271 Global)
0.1/yrCitation Velocity (#43312482 Global)
0.94Citation PageRank (#45329082 Global)
7Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

There are provided preflow periods t 11 , t 12 in which group III element materials TMG, TMA and TMI are not supplied from a group III element material container to a reaction region (reactor), while a group V element material PH 3 and an Mg dopant material are supplied from a group V element material container and a dopant material container to the reaction region (reactor) after an Mg-undoped group III-V compound semiconductor layer is crystallinically grown and before an Mg-doped group III-V compound semiconductor layer is crystallinically grown. According to the semiconductor manufacturing method, an Mg doping profile can be accurately controlled.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 2.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A semiconductor manufacturing method for crystallinically growing an Mg-doped group III-V compound semiconductor layer by transporting a group III element material, a group V element material and an Mg dopant material from a group III element material container, a group V element material container and a dopant material container, respectively, to a reaction region through a group III element material transport line, a group V element material transport line and a dopant material transport line and reacting the group III element material with the group V element material in the reaction region